| J4不锈钢及化学镀Ni-P和Ni-Cu-P镀层在液-固两相流中的冲刷腐蚀行为 |
| 方信贤; 白允强 ; 王章忠 |
| 南京工程学院材料工程学院; 南京 211167 |
|
| EROSION CORROSION BEHAVIOUR OF J4 STAINLESS STEEL AND ELECTROLESS PLATING COATINGS OF Ni–P AND Ni–Cu–P IN LIQUID–SOLID TWO–PHASE FLOW |
| FANG Xinxian; BAI Yunqiang; WANG Zhangzhong |
| School of Materials Science and Engineering; Nanjing Institute of Technology; Nanjing 211167 |
引用本文:
方信贤 白允强 王章忠. J4不锈钢及化学镀Ni-P和Ni-Cu-P镀层在液-固两相流中的冲刷腐蚀行为[J]. 金属学报, 2010, 46(2): 239-244.
.
EROSION CORROSION BEHAVIOUR OF J4 STAINLESS STEEL AND ELECTROLESS PLATING COATINGS OF Ni–P AND Ni–Cu–P IN LIQUID–SOLID TWO–PHASE FLOW[J]. Acta Metall Sin, 2010, 46(2): 239-244.
| [1] Zheng Y G, Yao Z M, Zag Y S, Wei X Y, Ke W. Acta Metall Sin, 2000; 36: 51
(郑玉贵, 姚治铭, 张玉生, 魏翔云, 柯 \ \ 伟. 金属学报, 2000; 36: 51)
[2] Zhang A F, Xing J D, Bao C G, Jia H R. Acta Metall Sin, 2002; 38: 521
(张安峰, 邢建东, 鲍崇高, 贾焕如. 金属学报, 2002; 38: 521)
[3] Wang Z Y, Zhu J H, Wang Z Z. Acta Metall Sin, 2007; 43: 648
(王再友, 朱金华, 王章忠. 金属学报, 2007; 43: 648)
[4] Zhang A F, Wang Y Y, Xing J D, Li C J. Acta Metall Sin, 2004; 40: 411
(张安峰, 王豫跃, 邢建东, 李长久. 金属学报, 2004; 40: 411)
[5] Perry J M, Neville A, Wilson V A, Hodgkiess T. Surf Coat Technol, 2001; 137: 43
[6] Man H C, Kwok C T, Yue T M. Surf Coat Technol, 2000; 132: 11
[7] Cui Z D, Man H C, Cheng F T, Yue T M. Surf Coat Technol, 2003; 162: 147
[8] Tam K F, Cheng F T, Man H C. Surf Coat Technol, 2002; 149: 36
[9] Stack M M, Purandare Y, Hovsepian P. Surf Coat Technol, 2004; 188–189: 556
[10] Song J F, Guo K M, Zhao Z H. Chin Nonferrous Met, 1998; 8: 379
(宋锦福, 郭凯铭, 赵子辉. 中国有色金属学报, 1998; 8: 379)
[11] Abdulsalam M, Shinohara T. Corrosion, 2003; 59: 4
[12] Jargelius–Petterson F F A, Pound B G. J Electrochem Soc, 1998; 145: 1462
[13] Pardo A, Merino M C, Coy A E, Viejo F, Arrabal R, Matykina E. Corros Sci, 2008; 50780
[14] Pardo A, Merino M C, Coy A E, Viejo F, Arrabal R, Matykina E. Corros Sci, 2008; 50: 1796
[15] Kemp M, Bennekom A V, Robinson F P A. Mater Sci Eng, 1995; A199: 183
[16] Balaraju J N, Anandan C, Rajam K S. Appl Surf Sci, 2005; 250: 88
[17] Zhao F X, Liu C, Zhang Z Z, Qiu T. Mater Protect, 2006; 39: 65
(赵芳霞, 刘琛, 张振忠, 邱泰. 材料保护, 2006; 39: 65)
[18] Abdel A A, Shehata A M. Appl Surf Sci, 2009; 255: 6652 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|