| NO2-和Cl-对模拟混凝土孔隙液中钢筋腐蚀行为的影响 |
| 乔 冰; 杜荣归; 陈雯; 朱燕峰; 林昌健 |
| 厦门大学化学化工学院固体表面物理化学国家重点实验室; 厦门 361005 |
|
| EFFECT OF NO2− AND Cl− ON THE CORROSION BEHAVIOR OF REINFORCING STEEL IN SIMULATED CONCRETE PORE SOLUTIONS |
| QIAO Bing; DU Ronggui; CHEN Wen; ZHU Yanfeng; LIN Changjian |
| State Key Laboratory for Physical Chemistry of Solid Surfaces; Department of Chemistry; College of Chemistry and Chemical Engineering; Xiamen University; Xiamen 361005 |
引用本文:
乔冰 杜荣归 陈雯 朱燕峰 林昌健. NO2-和Cl-对模拟混凝土孔隙液中钢筋腐蚀行为的影响[J]. 金属学报, 2010, 46(2): 245-250.
,
,
.
EFFECT OF NO2− AND Cl− ON THE CORROSION BEHAVIOR OF REINFORCING STEEL IN SIMULATED CONCRETE PORE SOLUTIONS[J]. Acta Metall Sin, 2010, 46(2): 245-250.
| [1] Kumar V. Corros Rev, 1988; 16: 317
[2] Zhang J, Lounis Z. Cem Concr Res, 2006; 36: 1312
[3] Du R G, Hu R G, Huang R S, Lin C J. Anal Chem, 2006; 78: 3179
[4] Huet B, LHostis V, Miserque F, Idrissi H. Electrochim Acta, 2005; 51: 172
[5] Kulakowski M P, Pereira F M, Dal Molin D C C. Constr Build Mater, 2009; 23: 1189
[6] Xu H, Liu Y, Chen W, Du R G, Lin C J. Electrochim Acta, 2009; 54: 4067
[7] Wu Q, Liu Y, Du R G, Lin C J. Acta Metall Sin, 2008; 44: 346
(吴 群, 刘 玉, 杜荣归, 林昌健. 金属学报, 2008; 44: 346)
[8] Hartt W H, Nam J. Corrosion, 2008; 64: 671
[9] Ryou J S, Ann K Y. Mag Concr Res, 2008, 60: 177
[10] Garces P, Saura P, Mendez A, Zornoza E, Andrade C. Corros Sci, 2008; 50: 498
[11] Gaidis J M. Cem Concr Compos, 2004; 26: 181
[12] Al–Amoudi O S B, Maslehuddin M, Lashari A N, Abdullah A A. Cem Concr Compos, 2003; 25: 439
[13] Tritthart J, Banfill P F G. Cem Concr Res, 2001; 31: 1093
[14] Nmai C K. Cem Concr Compos, 2004; 26: 199
[15] Song H W, Saraswathy V, Muralidharan S, Lee C H, Thangavel K. J Appl Electrochem, 2009; 39: 15
[16] Moreno M, Morris W, Alvarez M G, Duffo G S. Corros Sci, 2004; 46: 2681
[17] Sagues A A, Kranc S C, Moreno E I. Corros Sci, 1995; 37: 1097
[18] Neves R S, De Robertis E, Motheo A J. Electrochim Acta, 2006; 51: 1215
[19] Reffass M, Sabot R, Jeannin M, Refait P. Electrochim Acta, 2007; 52: 7599 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|