| 熔体处理对DZ40M返回合金力学性能的影响 |
| 杨金侠,郑启,桑志茹,郎海霞,孙晓峰,胡壮麒 |
| 中国科学院金属研究所, 沈阳 110016 |
|
| EFFECTS OF MELTING TREATMENTS ON THE MECHANICAL PROPERTIES OF REVERTED DZ40M ALLOY |
| YANG Jinxia, ZHENG Qi, SANG Zhiru, LANG Haixia, SUN Xiaofeng, HU Zhuangqi |
| Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
杨金侠 郑 启 桑志茹 郎海霞 孙晓峰 胡壮麒. 熔体处理对DZ40M返回合金力学性能的影响[J]. 金属学报, 2010, 46(12): 1511-1516.
,
,
,
,
,
.
EFFECTS OF MELTING TREATMENTS ON THE MECHANICAL PROPERTIES OF REVERTED DZ40M ALLOY[J]. Acta Metall Sin, 2010, 46(12): 1511-1516.
| [1] Li Z J. Master Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2005
(李志军. 中国科学院金属研究所硕士学位论文, 沈阳, 2005)
[2] Li Z J, Zhou L Z, Yao J. Mater Eng, 2005; (8): 24
(李志军, 周兰章, 姚俊. 材料工程, 2005; (8): 24)
[3] Huang X B. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 1997
(黄学兵. 中国科学院金属研究所博士学位论文, 沈阳, 1997)
[4] Yuan C, Wang T L. Acta Metall Sin, 2000; 36: 961
(袁超, 王铁利. 金属学报, 2000; 36: 961)
[5] Yuan C, Guo J T, Zang Z X, Lai W H, Liu Y M, Li H L. Trans Nonferrous Met Soc China, 2006; 16: 453
(袁超, 郭建亭, 藏志新, 赖万慧, 刘一鸣, 李洪亮. 中国有色金属学报, 2006; 16: 453)
[6] Zhou B, Zhao M H, Zhao J C. J Iron Steel Res, 2003; 15(7): 196
(周 波, 赵明汉, 赵京晨. 钢铁研究学报, 2003; 15(7): 196)
[7] Yu Q, Song J X, Wang D G, Qu S Y, Li Q. Mater Eng, 2006; (6): 10
(余乾, 宋尽霞, 王定刚, 曲士昱, 李青. 材料工程, 2006; (6): 10)
[8] Niu J P. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2002
(牛建平. 中国科学院金属研究所博士学位论文, 沈阳, 2002)
[9] Niu J P, Yang K N, Jin T, Sun X F, Guan H R, Hu Z Q. Acta Metall Sin, 2001; 37: 499
(牛建平, 杨克努, 金涛, 孙晓峰, 管恒荣, 胡壮麒. 金属学报, 2001; 37: 499)
[10] Niu J P, Yang K N, Sun X F, Jin T, Guan H R, Hu Z Q. Rare Met Mater Eng, 2003; 32: 63
(牛建平, 杨克努, 孙晓峰, 金涛, 管恒荣, 胡壮麒. 稀有金属材料与工程, 2003; 32: 63)
[11] Wang T L. PhD Thesis, Northeastern University, Shenyang, 2000
(王铁利. 东北大学博士学位论文, 沈阳, 2000)
[12] Yin F S, Guan H R, Sun X F, Hu Z Q. Acta Metall Sin, 2005, 41: 1190
(殷凤仕, 管恒荣, 孙晓峰, 胡壮麒. 金属学报, 2005, 41: 1190)
[13] Jiang W H. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 1999
(姜文辉. 中国科学院金属研究所博士学位论文, 沈阳, 1999)
[14] Yao X D. China Aeronautical Materials Handbook. Beijing: China Standard Press, 2001: 765
(姚向东. 中国航空材料手册. 北京: 中国标准出版社, 2001: 765) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|