| 预变形对低合金高碳钢超塑性变形行为的影响 |
| 张寒; 白秉哲; 方鸿生 |
| 清华大学材料科学与工程系先进材料教育部重点实验室; 北京 100084 |
|
| EFFECT OF PRESTRAIN ON THE SUPERPLASTIC DEFORMATION BEHAVIOR OF LOW-ALLOY HIGH-CARBON STEEL |
| ZHANG Han; BAI Bingzhe; FANG Hongsheng |
| Key Laboratory for Advanced Materials of Ministry of Education; Department of Materials Science and Engineering; Tsinghua University; Beijing 100084 |
引用本文:
张寒 白秉哲 方鸿生. 预变形对低合金高碳钢超塑性变形行为的影响[J]. 金属学报, 2009, 45(9): 1106-1110.
,
,
.
EFFECT OF PRESTRAIN ON THE SUPERPLASTIC DEFORMATION BEHAVIOR OF LOW-ALLOY HIGH-CARBON STEEL[J]. Acta Metall Sin, 2009, 45(9): 1106-1110.
| [1] Howe H M. The Metallurgy of Steel. 2nd ed, New York: Scientific Publishing Company, 1981: 16
[2] Sherby O D. ISIJ Int, 1999; 39: 637
[3] Sherby O D,Walser B, Young C M, Cady E M. Scr Metall, 1975; 9: 569
[4] Sherby O D, Oyama T, Kum D W, Walser B, Wadsworth J. J Met, 1985; 37(6): 50
[5] Oyama T, Sherby O D, Wadsworth J, Walser B. Scr Metall, 1984; 18: 799
[6] Tsuzaki K, Sato E, Furimoto S, Furuhara T, Maki T. Scr Mater, 1999; 40: 675
[7] Sato E, Furimoto S, Furuhara T, Tsuzaki K, Maki T. Mater Sci Forum, 1999; 304–306: 133
[8] Seto K, Kato T, Abe H. Mater Res Soc Symp Proc, 1990; 196: 99
[9] Matsumura Y, Yada H. Trans ISIJ, 1987; 27: 492
[10] Huang Q S, Li L F, Yang W Y, Sun Z Q. Acta Metall Sin, 2007; 43: 724
(黄青松, 李龙飞, 杨王玥, 孙祖庆. 金属学报, 2007; 43: 724)
[11] Hart E W. Acta Metall, 1967; 15: 351
[12] Nieh T G, Wadsworth J, Sherby O D. Superplasticity in Metals and Ceramics. New York: Cambridge University Press, 2005: 189
[13] Hu X H, Houtte P V, Leibeherr M, Walentek A, Seefeldt M, Vandekinderen H. Acta Mater, 2006; 54: 1029
[14] Song R, Ponge D, Raabe D, Kaspar R. Acta Mater, 2005; 53: 845
[15] Shin D H, Kim Y S, Lavernia E J. Acta Mater, 2001; 49: 2387
[16] Ivanisenko Y, Lojkowski W, Valiev R Z, Fecht H J. Acta Mater, 2003; 51: 5555 |
|