| 纳米CeO2p对镍基高温合金表面NiCoCrAlY激光熔覆涂层氧化行为的影响 |
| 王宏宇1;2;左敦稳1;王明娣3;邵建兵1 |
1. 南京航空航天大学江苏省精密与微细制造技术重点实验室; 南京 210016
2. 江苏大学机械工程学院; 镇江 212013
3. 苏州大学机电学院; 苏州 215021 |
|
| EFFECTS OF NANO–CeO2p ON OXIDATION BEHAVIORS OF NiCoCrAlY LASER CLADDING COATINGS ON Ni–BASED SUPERALLOYS |
| WANG Hongyu 1;2; ZUO Dunwen 1; WANG Mingdi 3; SHAO Jianbing 1 |
1. Jiangsu Key Laboratory of Precision and Micro–manufacturing Technology; Nanjing University of Aeronautics and Astronautics; Nanjing 210016
2. School of Mechanical Engineering; Jiangsu University; Zhenjiang 212013
3. College of Mechanical and Electrical Engineering; Soochow University; Suzhou 215021 |
引用本文:
王宏宇 左敦稳 王明娣 邵建兵. 纳米CeO2p对镍基高温合金表面NiCoCrAlY激光熔覆涂层氧化行为的影响[J]. 金属学报, 2009, 45(8): 971-977.
,
,
,
.
EFFECTS OF NANO–CeO2p ON OXIDATION BEHAVIORS OF NiCoCrAlY LASER CLADDING COATINGS ON Ni–BASED SUPERALLOYS[J]. Acta Metall Sin, 2009, 45(8): 971-977.
| [1] Liu C B, Lin F, Jiang X L. Chin J Nonferrous Met, 2007;17: 1
(刘纯波, 林 \ \ 峰, 蒋显亮. 中国有色金属学报, 2007; 17: 1)
[2] Li M S. Metal High Temperature Corrosion. Beijing: Metallurgical Industry Press, 2001: 248
(李美栓. 金属的高温腐蚀. 北京: 冶金工业出版社, 2001: 248)
[3] Wu Y N, Zhang G, Zhang B C, Feng Z C, Liang Y. J Mater Sci Technol, 2001; 17: 525
[4] Zhang Y P, Zhou Z R, Cheng J M, Ge Y L, Ma H. Surf Coat Technol, 1996; 76: 131
[5] Jin H M, Liu X J, Zhang L N. J Rare Earths, 2007; 25: 63
[6] Bao R L, Yu H J, Chen C Z. Surf Rev Lett, 2006; 13: 509
[7] Li M X, Zhang S H, Li H S, He Y Z, Yoon J H. J Mater Process Technol, 2008; 202: 107
[8] Wang H Y, Zuo D W, Li D S, Luo X Y, Wang M D, Zhu Y W. Chin Pat, ZL200710024996.X, 2009
(王宏宇, 左敦稳, 李多生, 骆心怡, 王明娣, 朱永伟. 中国专利, ZL200710024996.X, 2009)
[9] Wang H Y, Zuo D W, Sun Y L, Zhu Y W. Chin J Nonferrous Met, 2008; 18: 1089
(王宏宇, 左敦稳, 孙玉利, 朱永伟. 中国有色金属学报, 2008; 18: 1089)
[10] Wang H Y, Zuo D W, Jiao G M, You S X, Sun Y B. Chin Pat, CN200710135477.0, 2008
(王宏宇, 左敦稳, 焦光明, 于守鑫, 孙业斌. 中国专利, CN200710135477.0, 2008)
[11] Zhang Y J, Sun X F, Jin T, Guan H R, Hu Z L. Acta Metall Sin, 2003; 39: 189
(张玉娟, 孙晓峰, 金 涛, 管恒荣, 胡壮麟. 金属学报, 2003; 39: 189) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|