| 不锈钢0Cr18Ni10Ti焊接头高温、高应变率下的动态力学性能 |
| 许泽建;李玉龙;刘明爽;李朋洲;吴云刚 |
| 西北工业大学航空学院 |
|
| RESEARCH ON DYNAMIC MECHANICAL PROPERTIES OF 0Cr18Ni10Ti WELDED JOINT AT ELEVATED TEMPERATURES AND HIGH STRAIN RATES |
| XU Ze-Jian;;;; |
| 西北工业大学航空学院 |
引用本文:
许泽建; 李玉龙; 刘明爽; 李朋洲; 吴云刚 . 不锈钢0Cr18Ni10Ti焊接头高温、高应变率下的动态力学性能[J]. 金属学报, 2008, 44(1): 98-104 .
,
,
,
,
.
RESEARCH ON DYNAMIC MECHANICAL PROPERTIES OF 0Cr18Ni10Ti WELDED JOINT AT ELEVATED TEMPERATURES AND HIGH STRAIN RATES[J]. Acta Metall Sin, 2008, 44(1): 98-104 .
[1]Zhao Y X,Yang B,Li P Z.Nucl Power En9,2004;25(1): 45 (赵永翔,杨冰,李朋州.核动力工程,2004;25(1):45) [2]Zhang Z.Woodworking Mach,2002;(3):22 (张震.木工机床,2002;(3):22) [3]Guo W G.Acta Metall Sin,2006;42:463 (郭伟国.金属学报,2006;42:463) [4]Nemat-Nasser S,Guo W G.Mech Mater,2005;37:379 [5]Nemat-Nasser S,Guo W G,Kihl D P.J Mech Phys Solids, 2001;49:1823 [6]Nemat-Nasser S,Li Y L.Acta Mater,1998;46:565 [7]Gilat A,Wu X.Exp Mech,1994;34:166 [8]Lankford J.J Mater Sci,1981;16:1567 [9]Campbell J D,Ferguson W G.Philos Mag,1970;21:63 [10]Rosenfield A R,Hahn G T.Trans ASM,1966;59:962 [11]Seeger A.Philos Mag,1955;46:1194 [12]Lee W-S,Liu C-Y.Mater Sci Eng,2006;A426:101 [13]Su Y Q.Plastic Deformation Theory of Metal.Beijing: Metallurgical Industry Press,1995:145 (苏玉芹.金属塑性变形原理.北京:冶金工业出版社,1995:145) [14]Johnson G R,Cook W H.In:Proc 7th Int Syrup on Bal- listics,The Hague,Netherlands,American Defense Pre- paredness Association,1983:541 [15]Zerilli F J,Armstrong R W.J Appl Phys,1987;61:1816 [16]Steinberg D J,Cochran S G,Guinan M W.University of California Radiation Laboratory,UCRL-80465,Revision 2nd ed.,Lawrence Livermore National Laboratory,Liver- more,CA,1979 [17]Follansbee P S,Kocks U F.Acta Metall,1988;36:81 [18]Ren S Z,Zhang J J,Chen Z R,Shi Y F,Mao Z Q,Gao H W.Metallographic Map of Iron and Steel Shanghai: Shanghai Scientific and Technical Literature Press,2003: 588 (任颂赞,张静江,陈质如,施友方,毛照樵,高汉文.钢铁金相图谱.上海:上海科学技术文献出版社,2003:588) [19]Chen B L.Theory of Welding Metallurgy.Chapter 3, Beijing:Tsinghua University Press,1991 (陈伯蠡.焊接冶金原理.第3章,北京:清华大学出版社,1991) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|