| 往复挤压变形对ZK60镁合金力学性能的影响 |
| 王渠东;林金保;彭立明;陈永军 |
| 上海交通大学轻合金精密成型国家工程研究中心 |
|
| INFLUENCE OF CYCLIC EXTRUSION AND COMPRESSION ON THE MECHANICAL PROPERTIES OF ZK60 ALLOY |
| LIN Jin-bao;Wang Qudong;Peng Liming;Chen Yongjun |
| 上海交通大学轻合金精密成型国家工程研究中心 |
引用本文:
王渠东; 林金保; 彭立明; 陈永军 . 往复挤压变形对ZK60镁合金力学性能的影响[J]. 金属学报, 2008, 44(1): 55-58 .
,
,
,
.
INFLUENCE OF CYCLIC EXTRUSION AND COMPRESSION ON THE MECHANICAL PROPERTIES OF ZK60 ALLOY[J]. Acta Metall Sin, 2008, 44(1): 55-58 .
[1]Westengen H K.Light Met Age,2000;58(3-4):44 [2]Pekguleryuz M O.Mater Sci Forum,2000;350:131 [3]Dwain M,Magers A.Light Met Age,1996;54(9-10):60 [4]Yong M S,Clegg A J.J Mater Process Technol,2004;145: 134 [5]Yang Q,Ghosh A K.Acta Mater,2006;54:5159 [6]Avedesian M M,Baker H.ASM Specialty Handbook:Mag- nesium and Magnesium Alloys.Materials Park,OH:ASM International,1999:17 [7]Wang Y N,Huang J C.Acta Mater,2007;55:897 [8]Mukai T,Yamanoi M,Watanabe H,Higashi K.Scr Mater, 2001;45:89 [9]Stohr J F,Poirier J P.Philos Mag,1972;25:1313 [10]Obara T,Yoshinaga H,Morozumi S.Acta Mater,1973; 21:845 [11]Mabuchi M,Iwahashi H,Yanase K,Higashi K.Scr Mater, 1996;36:681 [12]KimW J,Hong S I,Kim Y S,Min S H,Jeong H T,Lee J D.Acta Mater,2003;51:3293 [13]Lin J B,Wang Q D,Chen Y J,Zhang L J,Ding W J. Trans Nonferrous Met Soc Chin,2006;16:206 [14]Barret C,Massalski T B.Structure of Metals.3rd ed., Oxford:Pergamon Press,1980:768 [15]Kim W J,Hong S I,Kim Y S.Acta Mater,2003;51:3293 [16]Mueller K,Mueller S.J Mater Process Technol,2007;187- 188:775 [17]Zhou H T,Ma C J,Zeng X Q,Ding W J.Mater Rev, 2003;17(11):16 (周海涛,马春江,曾小勤,丁文江.材料导报,2003;17(11):16) [18]Mueller S,Mueller K,Rosumek M,Reimers W.Alu- minium Int J,2006;82:327 [19]Spitzig W A,Richmond O.Acta Metall,1984;32:457 [20]Guo Q,Yan H G,Chen Z H,Zhang H.Acta Metall Sin, 2006;42:739 (郭强,严红革,陈振华,张辉.金属学报,2006;42:739) [21]Valiev R Z,Islamgaliev R K,Alexandrov I V.Prog Mater Sci,2000;45:103 [22]Meyers M A,Mishra A,Benson D J.Prog Mater Sci,2006; 51:427 [23]Christian J W,Mahajan S.Prog Mater Sci,1995;39:1 [24]Chen Z H,Yang C H,Huang C Q,Xia W J,Yan H G. Mater Rev,2006;20(8):107 (陈振华,杨春花,黄长清,夏伟军,严红革.材料导报,2006;20(8):107) [25]Perex-Prado M T,Valle J A,Ruano O A.Scr Mater, 2004;50:667 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|