| 立方晶体相界面位错的计算机模拟 |
| 陈会强 杨志刚 |
| 清华大学材料科学与工程系 |
|
| Computer--Based Simulation of Dislocations on Interfaces of Cubic Crystals |
| CHEN Huiqiang; Yang Zhigang |
| Department of Materials Science and Engineering; Tsinghua University |
引用本文:
陈会强; 杨志刚 . 立方晶体相界面位错的计算机模拟[J]. 金属学报, 2007, 43(7): 710-712 .
,
.
Computer--Based Simulation of Dislocations on Interfaces of Cubic Crystals[J]. Acta Metall Sin, 2007, 43(7): 710-712 .
[1]Zhang W Z.Acta Metall Sin,2002;38:785 (张文征.金属学报,2002;38:785) [2]Ye H Q.Structures and Characteristics of Interfaces in Materials.Beijing:Science Press,1999 (叶恒强.材料界面结构与特性.北京:科学出版社,1999) [3]Sutton A P,Balluffi R W.Interfaces in Crystalline Ma- terials.Oxford:Oxford University Press,1995 [4]Smith D A,Shiflet G.Mater Sci Eng,1987;86:67 [5]How J M.Interfaces in Materials.New York:John Wiley and Sons,1997 [6]Porter D A,Easterling K E.Phase Transformations in Metals and Alloys.New York:Chapman & Hall,1992 [7]Feng D.Metal Physics.Vol.Ⅰ,Beijing:Science Press, 1987:375 (冯端.金属物理学.第一卷,北京:科学出版社.1987:375) [8]Song Y J.Grian Boundaries and Strength of Metals, Xi'an:Xi'an Jiaotong University Press,1987 (宋余九.金属的晶界与强度.西安:西安交通大学出版社,1987) [9]Yu Y N.Principles of Physical Metallurgy.Beijing:Met- allurgical Industry Press,2000 (余永宁.金属学原理.北京:冶金工业出版社.2000) [10]Bollmann W.Crystal Defects and Crystalline Interfaces. Berlin:Springer,1970 [11]Bollmann W.Crystal Lattices,Interfaces,Matrices. Geneva:Bollmann,1982 [12]Spanos G.PhD Thesis,Carnegie-Mellon University, Pittsubrgh,PA,1989 [13]Lin D L.In:Li H D,Xiao J M eds.,Surface and In- terfaces in Materials,Beijing:Tsinghua University Press, 1990:165 (林栋梁.见:李恒德,肖纪美主编.材料表面与界面,北京:清华大学出版社,1990:165) [14]LUO C P,Liu Z Y.In:Li H D,Xiao J M eds.,Surface and Interfaces in Materials,Beijing:Tsinghua University Press,1990:201 (罗承萍,刘正义.见:李恒德,肖纪美主编,材料表面与界面,北京:清华大学出版社,1990:201) [15]Laird C,Aaronson H I.Acta Metall,1967;15:73 [16]Stephens D E,Purdy G R.Acta Metall,1975;23:1343 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|