| 试样厚度对共晶组织形态的影响 |
| 孟广慧;林鑫;杜立成;黄卫东 |
| 西北工业大学凝固技术国家重点实验室 (西北工业大学543#信箱) |
|
| INFLUENCE OF SAMPLE THICKNESS ON THE PATTERN FORMATION IN EUTECTIC SYSTEM |
| Guanghui Meng |
| 西北工业大学凝固技术国家重点实验室 (西北工业大学543#信箱) |
引用本文:
孟广慧; 林鑫; 杜立成; 黄卫东 . 试样厚度对共晶组织形态的影响[J]. 金属学报, 2007, 43(5): 459-464 .
,
,
,
.
INFLUENCE OF SAMPLE THICKNESS ON THE PATTERN FORMATION IN EUTECTIC SYSTEM[J]. Acta Metall Sin, 2007, 43(5): 459-464 .
[1] Trivedi R, Kurz W. In: Stefanescu M A, Abbaschian G J J, eds., Solidification Processing of Eutectic Alloys, War- rendale, PA: AIME, 1988: 3 [2] Jackson K A, Hunt J D. Trans AIME, 1966; 236: 1129 [3] Sato T, Sayama Y. J Cryst Growth, 1974; 22: 259 [4] Magnin P, Trivedi R. Acta Metall Mater, 1991; 39: 453 [5] Zheng L L, Larson D J, Zhang J H. J Cryst Growth, 2000; 209: 110 [6] Catalina A V, Sen S, Stefanescu D M. Metall Mater Trans, 2003; 34A: 383 [7] Trivedi R, Magnin P, Kurz W. Acta Metall, 1987; 35: 974 [8] Flolch R, Plapp M. Phys Rev, 2003; 68E: 010602(R) [9] Akamatsu S, Bottin-Rousseau S, Faivre G. Phys Rev Lett, 2004; 93: 175701 [10] Mergy J, Faivre G, Guthmann C, Mellet R. J Cryst Growth, 1993; 134: 353 [11] Seetharaman V, Trivedi R. Metall Trans, 1988; 19A: 2955 [12] Jordan R M, Hunt J D. Metall Trans, 1972; 3: 1385 [13] Juarez-Hernandez A, Jones H. Metall Mater Trans, 2000; 31A: 327 [14] Dunning W J. J Phys Chew. Solids, 1961; 18: 21 [15] Tiller W A, Jackson K A, Rutter J W, Chalmers B. Acta Metall, 1953; 1: 428 [16] Caroli B, Caroli C, Faivre G, Mergy J. J Cryst Growth, 1992; 118: 135 [17] Faivre G. Phys Rev, 1992; 45A: 7320 [18] Seetharaman V, Fabietti L M, Trivedi R. Metall Trans, 1989; 20A: 2567 [19] Kassner K, Misbah C. Phys Rev, 1991; 44A: 6533 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|