| Gasar工艺下难以制得藕状多孔Al的原因分析 |
| 张华伟;李言祥;刘源 |
| 先进成形制造教育部重点实验室;清华大学机械工程系 |
|
| Difficulty in Fabricating Lotus-type Porous Al by Gasar Process |
| Hua-Wei ZHANG;; |
| 先进成形制造教育部重点实验室;清华大学机械工程系 |
引用本文:
张华伟; 李言祥; 刘源 . Gasar工艺下难以制得藕状多孔Al的原因分析[J]. 金属学报, 2007, 42(1): 11-16 .
,
,
.
Difficulty in Fabricating Lotus-type Porous Al by Gasar Process[J]. Acta Metall Sin, 2007, 42(1): 11-16 .
[1]Shapovalov V I.US Pat,5,181,549,1993 [2]Liu Y,Li Y X,Zhang H W.Acta Metall Sin,2004;40: 1121 (刘源,李言祥,张华伟.金属学报, 2004;40:1121) [3]Ikeda T,Nakajima H.J Jpn Foundry Eng Soc,2002;74: 812 (池田辉之,中(?)英雄铸造工学, 2002;74:812) [4]Nakajima H,Hyun S K,Ohashi K,Ota K,Murakami K. Coll Surf, 2001;A179:209 [5]Suematsu Y, Hyun S K, Nakajima H. J Jpn lnst MEt, 2004;68:257 (末松佳记,玄丞均,中(?)英雄.日本金属学会志, 2004; 68: 257) [6]Nakahata T,Nakajima H.Mater Trans,2005;46:587 [7]Hyun S K,Nakajima H.Mater Trans,2002;43:526 [8]Hyun S K, Nakajima H.Adv Eng Mater,2002;4:741 [9]Hyun S K, Ikeda T, Nakajima H.Sci Technol Adv Mater, 2004;5:201 [10]Ikeda T,Aoki T,Nakajima H.Metall Mater Trans,2005; 36A:77 [11]Ikeda T,Tsukamoto M,Nakajima H.Mater Trans,2002; 43:2678 [12] Kashihara M,Hyun S K,Yonetani H,Kobi T,Nakajima H.Scr Mater,2006;54:509 [13] Kujime T,Hyun S K,Nakajima H.Metall Mater Trans, 2006;37A:393 [14] Nakahata T,Nakajima H. Mater Sci Eng,2004;A384: 373 [15] Nakajima H,Ikeda T,Hyun S K.Adv Eng Mater,2004; 6:377 [16] Shapovalov V I.In:Lavernia E J,Gungor M N,eds., Microstructural Design by Solidification Processing,War- rendale,PA:The Minerals,Metals&Materials Society, 1992:207 [17] Manchester F D.Phase Diagrams of Binary Hydrogen Al- loys.Materials Park,OH:ASM International,2000:4 [18] Li Y X.Principle of Materials Processing.Beijing:Ts- inghua University Press,2005:188 (李言祥.材料加工原理.北京:清华大学出版社,2005:188) [19] An G Y.Formation Theory of Casting.Beijing:China Machine Press,1989:173 (安阁英.铸件形成理论.北京:机械工业出版社, 1989:173) [20] Brandes E A,Brook G B.Smithells Metals Reference Book.7th Ed., Boston:Butterworth-Heinemann I,td., 1992:12-5 [21] Liu Y, Li Y X.Scr Mater, 2003;49:379 [22] Beer S Z.Liquid Metals: Chemistry and Physics.New York:Marcel Dekker Inc., 1972:186 [23] Liu Y,Li Y X,wan J,Zhang H W.In:Nakajima H,Kane- take N.eds., Proc MetFoam 2005,Sendai:The Japan In- stitute of Metals, 2006:24l [24] Hyun S K,Nakajima H.Mater Lett,2003;57:3149 [25] Zhang H W,Li Y X,Liu Y.Acta Metall Sin,2006;42: 1171 (张华伟,李言祥,刘源. 金属学报,2006;42:1171) [26] Paradies C J,Tobin A,walla J. Mater Res Soc Symp Proc, 1998;52l:297 [27]Liu Y,Li Y X.Trans Nonferrous Met Soc Chin,2003;l3: 830 [28] Apprill J M,Poirier D R,Maguire M C.Mater Res Soc Symp Proc,1998;521:291 [29] Liu Y,Li Y X,Wan J,Zhang H W.Mater Sci Eng,2005; A402:47 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|