| Zr 含量对Ti-1100 合金中硅化物析出的影响 |
| 徐锋; 李阁平; 杨锐; Mesut Varlioglu; Philip Nash |
| 中国科学院金属研究所; 沈阳 110016 |
|
| EFFECT OF ZIRCONIUM CONTENT ON PRECIPITATION OF SILICIDE IN TI-1100 ALLOY |
| XU Feng; LI Geping; YANG Rui M. Varlioglu; P. Nash |
| Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
徐锋; 李阁平; 杨锐; Mesut Varlioglu ; Philip Nash . Zr 含量对Ti-1100 合金中硅化物析出的影响[J]. 金属学报, 2006, 42(7): 770-776 .
,
,
,
,
.
EFFECT OF ZIRCONIUM CONTENT ON PRECIPITATION OF SILICIDE IN TI-1100 ALLOY[J]. Acta Metall Sin, 2006, 42(7): 770-776 .
[1] Lee D H,Nam S W,Choe S J. Scr Metall, 1999; 40: 265 [2] Weinem D, Kumpfert J, Peters M, Kaysser W A. Mater Sci Eng, 1996; A206: 55 [3]ьорисов E A ed., Translated by Chen S Q. Metallography of Titanium Alloys. Beijing: National Defence Industry Press, 1980: 4 (ьорисовE A著.陈石卿译.钛合金金相学.北京: 国防工业出版社,1980:4) [4] Yan Y, Han D, Cao M Z. Chin J Mater Res, 1996; 10:587 (颜 莹,韩 东,曹名洲.材料研究学报, 1996;10:587) [5] Chen W F, Shi Y F. Rare Mater Eng, 1999; 28: 323 [6] Rosenberger A H,Madsen A,Ghonem H. J Mater Eng Perform, 1995; 2: 182 [7] Madsen A, Ghonem H. Mater Sci Eng, 1994; A177: 63 [8] Boyer R, Weksch G, Collings E W. Materails Properties Handbook:Titanium Alloys.Materials Park,OH: AMS,1994: 411 [9] Cui W F,Liu C M, Zhou L,Luo G Z.Mater Sci Eng, 2002; A323: 192 [10] Singh A K,Ramachandra C.J Mater Sci,1997; 32: 229 [11] Ramachandra C, Singh V.Metall Trans,1992; 23A:689 [12] Bulanova M, Firstov S,Gornaya I,Miracle D. J Alloys Compd, 2004; 384: 106 [13] Weinem D,Kumpfert J,Peters M,Kaysser W A.Mater Sci Eng, 1996; A206: 55 [14] Lutjering G,Williams.Titaniu.Heidelberg:Springer-Verlag 2003: 232 [15] Cui Z Q. Metallurgy and Heat Treatment. Beijing: China Machine Press, 2000: 138 (崔忠圻.金属学与热处理.北京:机械工业出版社,2000:138) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|