| 退火与淬火态钛合金中beta相体积分数的近似计算 |
| 屈 华 刘伟东 刘志林 |
| 辽宁工学院材料与化学工程学院 |
|
| APPROXIMATE CALCULATION OF VOLUME FRACTION OF PHASES WITH QUENCHED AND ANNEALED STRUCTURE IN a+b AND b TITANIUM ALLOYS |
| Hua Qu |
| 辽宁工学院材料与化学工程学院 |
引用本文:
屈华; 刘伟东; 刘志林 . 退火与淬火态钛合金中beta相体积分数的近似计算[J]. 金属学报, 2006, 42(4): 374-378 .
,
,
.
APPROXIMATE CALCULATION OF VOLUME FRACTION OF PHASES WITH QUENCHED AND ANNEALED STRUCTURE IN a+b AND b TITANIUM ALLOYS[J]. Acta Metall Sin, 2006, 42(4): 374-378 .
[1] Nathal M V, Ebert L J. Metall Trans, 1985; 16A: 1849 [2] Glatzel U, Feller-Kniepmeier M. Scr Metall Mater, 1991; 25: 1845 [3] Melow T, Zhu J W, Wahi R P. Z Metallkd, 1994; 85: 9 [4] Lempke H, Wang Y, Mukherji D, Chen W, Wiedenmann A, Wahi R P. Z Metallkd, 1994; 87: 286 [5] Schulze C, Feller-Kniepmeier M. Scr Mater, 2001; 44: 731 [6] Glatzel U. Microstructure and Internal Strains of Unde- formed and Greep Deformed Samples of a Nickel-base Su- peralloy. Berlin: Verlag Dr KSster, 1994: 10 [7] Schmidt R, Feller-Kniepmeier M. Metall Trans, 1992; 23A: 745 [8] Schmidt R, Feller-Kniepmeier M. Scr Metall Mater, 1992; 26: 1919 [9] Harada H, Yamazaki M, Koizumi Y, Sakuma N, Furuya N, Kamiya H. High Temperature Alloys for Gas Turbines 1982, Liege, Belgium: D.Reidel Press Co., 1982: 721 [10] Liu Y, Peng Z F, Ren Y Y, Wang Y Q. Acta Metall Sin, 2002; 38: 131 (刘艳,彭志方,任遥遥,王延庆.金属学报,2002;38:131) [11] Liu Y, Peng Z F. Acta Metall Sin, 2003; 39: 22 (刘艳,彭志方.金属学报,2003;39:22) [12] Zhang B C. Nonferrous Metal and Heat Treat. Xi'an: North-Western Polytechnical University Press, 1993: 93 (张宝昌.有色金属及其热处理.西安:西北工业大学出版社, 1993:93) [13] Zhou Y B. Casting Conspectus of Titanium Alloys. Beijing: Aerospace Industry Press, 2000: 16 (周彦邦.钛合金铸造概论.北京:航空工业出版社,2000:16) [14] Wang G S. Chin J Rare Met, 1995; 19: 352 (王桂生.稀有金属,1995;19:352) [15] Zhang X D, Wiezorek J M K, Baeslack W A III, Evans D J, Fraser H L. Acta Mater, 1998; 46: 4486 [16] Sha A X, Wang Q R, Li X W. Chin J Rare Met, 2004; 28: 239 (沙爱学,王庆如,李兴无.稀有金属, 2004;28:239) [17] Ning X L. Rare Met Mater Eng, 2000; 5: 331 (宁兴龙.稀有金属材料与工程, 2000;5:331) [18] Mao P L. Shanghai Steel Res, 1995; 3: 52 (毛彭龄.上海钢铁研究, 1995;3:52)? |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|