| Zr41.25Ti13.75Ni10Cu12.5Be22.5多孔块体非晶合金的制备 |
| 任英磊 索忠源 邱克强 |
| 沈阳工业大学材料科学与工程学院 |
|
| FABRICATION OF Zr41.25Ti13.75Ni10Cu12.5Be22.5 BULK METALLIC GLASS FOAM |
| QIU K Q |
| 沈阳工业大学材料科学与工程学院 |
引用本文:
任英磊; 索忠源; 邱克强 . Zr41.25Ti13.75Ni10Cu12.5Be22.5多孔块体非晶合金的制备[J]. 金属学报, 2006, 42(4): 379-382 .
,
,
.
FABRICATION OF Zr41.25Ti13.75Ni10Cu12.5Be22.5 BULK METALLIC GLASS FOAM[J]. Acta Metall Sin, 2006, 42(4): 379-382 .
[1] Pan M X, Wang W H. Physics, 2002; 31: 453 (潘明祥,汪卫华.物理,2002;31:453) [2] http://www.liquidmetal.com/applications/ [3] Qiu K Q, Wang A M, Zhang H F, Ding B Z, Hu Z Q. Intermetallica, 2002; 10: 1283 [4] Qiu K Q, Wu X F, Wang A M, Zhang H F, Hu Z Q. Metall Mater Trans, 2003; 34A: 1147 [5] Schroers J, Veazey C, Johnson W L. Appl Phys Lett, 2003; 82: 370 [6] Brothers A H, Dunand D C. Appl Phys Lett, 2004; 84: 1108 [7] Apfel R E, Qiu N. J Mater Res, 1996; 11: 2916 [8] Wada T, Inoue A. Mater Trans, 2004; 45: 2761 [9] Wada T, Inoue A. Mater Trans, 2003; 44: 2228 [10] Brothers A H, Scheunemann R, DeFouw J D, Dunand D C. Scr Mater, 2005; 52: 33 [11] Peker A, Johnson W L. Appl Phys Lett, 1993; 63: 2342 [12] Conner R D, Johnson W L, Paton N E, Nix W D. J Appl Phys, 2003; 94: 904 [13] Liu P S. Introduction to Cellular Materials. Beijing: Tsinghua University Press, 2004: 300 (刘培生.多孔材料引论.北京:清华大学出版社,2004:300) [14] Conner R D, Dandliker R B, Johnson W L. Acta Mater, 1998; 46: 6089 [15] Marchi S C, Brothers A H, Dunand D C. Mater Res Soc Symp Proc, 2003; 754: CC1.8.1 [16] Qiu K Q. PhD Dissertation, Institute of Metal Research, The Chinese Academy of Sciences, Shenyang, 2002 (邱克强.中国科学院金属研究所博士学位论文,沈阳,2002) [17] Dandliker R B, Conner R D, Johnson W L, J Mater Res, 1998; 13: 2896 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|