| 氢对锆基块体非晶合金热膨胀系数和有效原子作用势的影响 |
| 彭德林 沈 军 孙剑飞 陈玉勇 |
| (哈尔滨工业大学材料科学与工程学院; 哈尔滨 150001) |
|
引用本文:
彭德林; 沈军; 孙剑飞; 陈玉勇 . 氢对锆基块体非晶合金热膨胀系数和有效原子作用势的影响[J]. 金属学报, 2005, 41(8): 835-838 .
[1] Koster U, Zander D. Mater Sci Forum, 2000; 343-346: 203 [2] Suh D, Dauskardt R H. Scr Mater, 2000; 42: 233 [3] Zander D, Leptien H, Koster U, Eliaz N, Eliezer D. J Non-Cryst Solids, 1999; 250-252: 893 [4] Peng D L, Shen J, Sun J F, Chen Y Y. Acta Metall Sin, 2003; 39: 1081 (彭德林,沈军,孙剑飞,陈玉勇.金属学报,2003;39:1081) [5] Peng D L, Shen J, Sun J F, Chen D M, Chen Y Y. Chin J Nonferrous Met, 2003; 13: 846 (彭德林,沈军,孙剑飞,陈德民,陈玉勇.中国有色金属学 报, 2003;13:846) [6] Peng D L, Shen J, Sun J F, Chen Y Y. J Mater Sci Tech- nol, 2004; 20: 157 [7] Chen C L. Solid Physics. Xi'an: Northwestern Polytech- nical University Press, 2000: 37 (陈长乐.固体物理学.西安;西北工业大学出版社,2000:37) [8] Porscha B, Neuhauser H. Phys Status Solidi, 1994; 186B: 119 [9] Fu L. Met Fund Mater, 1998; 5: 39 (富莉.金属功能材料, 1998;5:39) [10] Jing Q, Liu R P, Li G, Wang W K. Scr Mater, 2003; 49: 111 [11] Wang H W, Wei Q, Friedrich S. J Phys Rev, 1998; 57B: 8211 [12] Lu I R, Gorier G P, Fecht H J, Willnecker R. J Non-Cryst Solids, 2000; 274: 294 [13] Yu B, Chen W J, Zheng G Z, Lin G M. Ada Sci Nat Univ Sunyatseni, 2001; 40: 120 (余斌,陈文军,郑国祯,林光明.中山大学学报(自然科学 版),2001;40:120) [14] Suh D, Dauskardt R H. Scr Mater, 2000; 42: 233m |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|