| Sm2Co17基高温稀土永磁材料的显微结构与磁性 |
| 李丽娅 易健宏 黄伯云 彭元东 |
| 中南大学粉末冶金国家重点实验室; 长沙 410083 |
|
引用本文:
李丽娅; 易健宏; 黄伯云; 彭元东 . Sm2Co17基高温稀土永磁材料的显微结构与磁性[J]. 金属学报, 2005, 41(8): 791-794 .
[1] Abhyankar A C, Gopalan R, Singh A K. J Mater Sci, 2004; 39: 3433 [2] Panagiotopoulos I, Gjoka M, Niarchos D. J Magn Magn Mater, 2004; 279: 389 [3] Kim A S. US Pat, No. 577 S79 6, 1998 [4] Li L Y, Yi J H, Zeng Q L. Chin J Mater Res, 2003; 17: 45 (李丽娅,易健宏,曾庆灵.材料研究学报, 2003;17:45) [5] Yan A R, Sun Z G, Han B S, Shen B G. J Mater Res, 2002; 17: 648 [6] Goll D, Kronmuller H. Naturwissenschaften, 2000; 87: 423 [7] Xiong X Y, Ohkubo T, Koyama T. Ada Mater, 2004; 52: 737 [8] Kronmuller H, Goll D. Scr Mater, 2002; 47: 545 [9] Yan A, Gutfeisch O, Handstein A. J Appl Phys, 2003; 93: 7975 [10] Matthiasa T, Zehetnera G, Fidler J. J Magn Magn Mater, 2002; 242-245: 1353 [11] Zhang Y, Cortel-Real M M, Hadjipanayis G C. J Appl Phys, 2000; 187: 6722 [12] Zhang Y, Tang W, Hadjipanayis G C. IEEE Trans Magn, 2001; 37: 2525 [13] Zhou S Z. Rare-Earth Permanent Magnets and Their Application. 2nd ed., Beijing: Metallurgical Industry Press, 1998: 87 (周寿增.稀土永磁材料及其应用.第2版,北京:冶金工业出 版社, 1998:87)z |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|