					引用本文:
						|  |  
    					|  |  
    					| 电磁离心铸造NiAl共晶合金的显微组织和力学性能 |  
						| 肖 旋  郭建亭 于海朋 |  
					| 中国科学院金属研究所;沈阳 110016 |  
						|  |  
								肖旋; 郭建亭; 于海朋                                                                                                                                                                                                                                             . 电磁离心铸造NiAl共晶合金的显微组织和力学性能[J]. 金属学报, 2005, 41(5): 507-510       .	
																												 
					
						| 
								
									|  
          
          
            
                         
            
									            
									                
																														  
																| [1] Johnson D R, Chen X F, Oliver B F, Noebe R D, Whit tenberger J D. Intermetallics, 1995; 3: 99 [2] Chen X F, Johnson D R, Noebe R D, Oliver B F. J Mater Res, 1995; 10: 1159
 [3] Darolia R. Intermetallics, 2000; 8: 1321
 [4] Raj S V, Locci I E, Whittenberger J D. In: Hemker K J, Dimiduk D M, Clemens H, Darolia R, Inui H, Larsen J M, Sikka V K, Thomas M, Whittenberger J D eds., Structural Intermetallics 2001, TMS, 2001: 785
 [5] Whittenberger J D, Locci I E, Raj S V, Salem J A. Metall Mater Trans, 2002; 33A: 1385
 [6] Cui C Y, Guo J T, Qi Y H, Ye H Q. Mater Trans, 2001; 42: 1700
 [7] Cui C Y, Guo J T, Qi Y H, Ye H Q. Intermetallics, 2002; 10: 1001
 [8] He Y L, Yang Y S, Hu Z Q. Mater Rev, 2000; 14(7): 3 (贺幼良,杨院生,胡壮麒.材料导报, 2000;14(7):3)
 [9] Qiu Y Q, Wang X, Jia G L, Gao Y Y, Yang H C. J North easten Univ (Natural Sci), 2000; 21:181 (邱以清,王溪,贾光霖,高允彦,杨洪才.东北大学学报(自 然科学版),2000;21:181)
 [10] Guo D Y, Yang Y S, Tong W H, Hua F A, Cheng G F, Hu Z Q. Acta Metall Sin, 2003; 39: 914 (郭大勇,杨院生,童文辉,花福安,程根发.胡壮麒.金属学 报. 2003;39:914)
 [11] Lin G, Yang Y S, Hua F A, Guo D Y, Hu Z Q, Acta Metall Sin, 2003; 39: 1233 (林刚,杨院生,花福安,郭大勇,胡壮麒.金属学报.2003; 39:1233)
 [12] Chen Y X, Cui C Y, He L L, Guo J T, Li D X. Acta Metall Sin, 1999; 35: 897 (陈玉喜,崔传勇,贺连龙,郭建亭,李斗星.金属学报,1999; 35:897)
 [13] Walston W S, Darolia R. In: Hemker K J, Dimiduk D M, Clemens H, Darolia R, Inui H, Larsen J M, Sikka V K, Thomas M, Whittenberger J D, eds., Structural Intermetallics 2001, TMS, 2001: 735
 |  
             
												
											    	
											        	|  | Viewed |  
											        	|  |  |  
												        |  | Full text 
 | 
 
 |  
												        |  |  |  
												        |  | Abstract 
 | 
 |  
												        |  |  |  
												        |  | Cited |  |  
												        |  |  |  |  
													    |  | Shared |  |  
													    |  |  |  |  
													    |  | Discussed |  |  |  |  |