| 柱状晶Al在冷轧过程中微观组织演变的定量表征: II 微观分裂 |
| 吴桂林 刘 伟 A. Godfrey 刘 庆 |
| 清华大学材料科学与工程系; 北京100084 |
|
| MICROSTRUCTURAL EVOLUTION OF COLUMNAR GRAIN Al DURING COLD ROLLING II. Mircoscopic Subdivision |
| WU Guilin; LIU Wei; A. Godfrey; LIU Qing |
| Department of Materials Science and Engineering; Tsinghua University; Beijing 100084 |
引用本文:
吴桂林; 刘伟; A.Godfrey; 刘庆 . 柱状晶Al在冷轧过程中微观组织演变的定量表征: II 微观分裂[J]. 金属学报, 2004, 40(7): 709-715 .
,
,
,
.
MICROSTRUCTURAL EVOLUTION OF COLUMNAR GRAIN Al DURING COLD ROLLING II. Mircoscopic Subdivision[J]. Acta Metall Sin, 2004, 40(7): 709-715 .
[1] Wu G L, Godfrey A, Liu Q. Acta Metall Sin, 2004; 40:699 [2] Hansen N, Juul Jensen D. Proc R Soc Lond A, 1999; 357:1447 [3] Liu Q, Hansen N. Proc R Soc Lond A, 1998; 454: 2555 [4] Liu Q, Maurice C, Driver D, Hansen N. Metall MaterTrans, 1998; 29A: 2333 [5] Akef A, Driver J H. Mater Sci Eng, 1991; A132: 245 [6] Basson F, Driver J H. Acta Mater, 2000; 48: 2101 [7] Li Z J, Liu Q. Mater Sci Eng, 2002; A338: 237 [8] Kuhlmann-Wilsdorf D, Hansen N. Scr Metall, 1991; 25:1557 [9] Bay B, Hansen N, Hughes D A, Kuhlmann-Wilsdorf D.Acta Metall Mater, 1992; 40: 205 [10] Hughes D A, Hansen N. Metall Trans, 1993; 24A: 2021 [11] Liu Q, Juul Jensen D, Hansen N. Acta Mater, 1997; 46:5819 [12] Huang X, Hansen N. Scr Mater, 1997; 37: 1 [13] Huang X. Scr Mater, 1998; 38: 1697 [14] Wert J, Liu Q, Hansen N. Acta Mater, 1995; 43: 4153 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|