| 磷含量对细晶镍基GH4133合金力学性能的影响 |
| 孙文儒; 郭守仁; 孟晓娜; 李娜; 胡壮麒 |
| 中国科学院金属研究所; 沈阳110016 |
|
| Effect of Phosphorus on Mechanical Properties of Fine-Grained GH4133 Nickel Base Superalloy |
| SUN Wenru; GUO Shouren; MENG Xiaona; LI Na; HU Zhuangqi |
| Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
孙文儒; 郭守仁; 孟晓娜; 李娜; 胡壮麒 . 磷含量对细晶镍基GH4133合金力学性能的影响[J]. 金属学报, 2004, 40(5): 477-482 .
,
,
,
,
.
Effect of Phosphorus on Mechanical Properties of Fine-Grained GH4133 Nickel Base Superalloy[J]. Acta Metall Sin, 2004, 40(5): 477-482 .
[1] Hu Z Q, Sun W R, Guo S R. Acta Metall Sin (Eng Lett), 1996; 9:443 [2] Sun W R, Guo S R, Lu D Z, Hu Z Q. Metall Mater Trans, 1997; 28A: 649 [3] Cao W D, Kennedy R L. In: Loria E A, ed., Superalloys 718, 625 and Various Derivatives, Warrendale, PA: TMS-AIME, 1994:463 [4] Sun W R, Guo S R, Hu Z Q. Mater Sci Eng, 1998; A247: 173 [5] Cao W D, Kennedy R L. In: Kissinger R D, Deye D J, Anton D L, Cetel A D, Nathal M V, Pollock T M, Woodford D A, eds., Superalloys 1996, Warrendale, PA: TMS- ??AIME, 1996:589 [6] Sun W R, Guo S R, Lu D Z, Li Z C, Tong B Y, Hu Z Q. In: Hanada S, Zhong Z, Nam S W, Wright R N, eds., 4th Pacific Rim Int Conf on Advanced Materials and Processing (PRICM4) , The Japan Institute of Metals, 1996:2719 [7] Song H W. PhD Thesis, Institute of Metal Research, The Chinese Academy of Sciences, Shenyang, 1999(宋洪伟.中国科学院金属研究所博士学位论文,沈阳,1999) [8] Hu Z Q, Sun W R, Guo S R, Lu D Z. J Iron Steel Res, 2002; (Spec Issue): 337. In: Xin P, Hu L, Ju D Y, eds., The 3rd Int Forum on Advanced Materials Science and Technology, Anshan, Anshan University of Science and Technology, 2002 [9] Editing Board of China Aeronautical Materials Handbook. China Aeronautical Materials Handbook. Vol.2: Wrought and Cast Superalloys. 2nd ed., Beijing: Standards Press of China, 2002:293(中国航空材料手册编辑委员会.中国航空材料手册(第2卷:变形高温合金铸造高温合金).第2版,北京:中国标准出版社,2002:293). |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|