| SiCw/Al复合材料高温再结晶行为的X射线衍射分析 |
| 姜传海 吴建生 王德尊 |
| 上海交通大学材料科学与工程学院高温材料及高温测试教育部重点实验室 |
|
| X--Ray Diffraction Analysis for the Recrystallization Behavior Of SiCw/Al Composite at High Temperature |
| JIANG Chuanhai; WU Jiansheng;WANG Dezun |
引用本文:
姜传海; 吴建生; 王德尊 . SiCw/Al复合材料高温再结晶行为的X射线衍射分析[J]. 金属学报, 2004, 40(10): 1023-1026 .
,
,
.
X--Ray Diffraction Analysis for the Recrystallization Behavior Of SiCw/Al Composite at High Temperature[J]. Acta Metall Sin, 2004, 40(10): 1023-1026 .
[1] Lloyd D J. Int Mater Rev, 1994; 39(1) : 1 [2] Huda M D, Hashmi M S J, Ei-Baradie M A. Key EngMater, 1995; 104-107(Part Ⅰ): 37 [3] Doherty R D, Hughes D A, Humphreys F J. Mater SciEng, 1997; A238: 219 [4] Clyne T W, Withers P J. An Introduction to Metal MatrixComposites. Cambridge: Cambridge University Press,1993: 383 [5] Liu Y L, Jensen D J, Hansen N. Metall Trans A, 1992; 23A: 807 [6] Teng F E, Wang Y M, Jiang X L. X-ray Structure Analysis and Property Representation of Materials. Beijing: Science Press, 1997: 177(滕凤恩,王煜明,姜小龙.X射线结构分析与材料性能表征.北京:科学出版社,1997:177) [7] Pan J S, Quan J M, Tian M B. Fundamentals of Materials Science. Beijing: Tsinghua University Press, 2002: 513(潘金生,全健民,田民波.材料科学基础.北京:清华大学出版社,2002:513) [8] Sherby O D, Burke P M. Prog Mater Sci, 1966: 13, 323 [9] Jiang C H, Wang D Z, Yao C K. J Mater Sci Lett, 2000:19: 1285 [10] Jiang C H, Wu J S, Wang D Z. Trans Nonferrous Met SocChin, 2001: 11: 729; |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|