| Ti-6Al-4V合金在真空中的干滑动磨损行为 |
| 刘勇 杨德庄 何世禹 |
| 哈尔滨工业大学空间材料与环境工程实验室 150001 |
|
引用本文:
刘勇; 杨德庄; 何世禹 . Ti-6Al-4V合金在真空中的干滑动磨损行为[J]. 金属学报, 2003, 39(7): 711-714 .
[1] Kragelskii I V, Lyubarskii I M, Guslyakov A A, Troynovskay G I, Udovenko V F. Friction and Wear in Vacuum. Moscow: Mashinostroenie, 1973: 10(1973: 10) [2] Landman U, Luedtke W D, Ringer E M. Wear, 1992; 153: 3 [3] Mishina H. Wear, 1992; 152: 99 [4] Bozet J--L. Wear, 1993; 162--164: 1025 [5] Dong H, Shi W, Bell T. Wear, 1999; 225--229: 146 [6] Dong H, Bell T. Wear, 1999: 225--229: 874 [7] Budinski K G. Wear, 1991; 151: 2O3 [8] Lebedeva I L, Presnyakova G N. Wear, 1991; 148: 203 [9] Panin V, Kolubaev A, Tarasov S, Popov V. Wear, 2001; 249: 860 [10] Kuhlmann--Wilsdorf D. Wear, 1996; 200: 8 [11] Popov P, Kolubaev A V. Technol Phys Lett, 1996; 22(13) : 37 |
|