| 内高压成形起皱行为的研究 |
| 王小松; 苑世剑; 王仲仁 |
| 哈尔滨工业大学材料科学与工程学院; 哈尔滨 150001 |
|
引用本文:
王小松; 苑世剑; 王仲仁 . 内高压成形起皱行为的研究[J]. 金属学报, 2003, 39(12): 1276-1280 .
[1] Yuan S J, Wang Z R. Chin Mech Eng, 2002; 13:783 [2] Dohmann F, Hartl C. J Mater Proc Technol, 1997; 71:174 [3] Altan T, Jirathearanat S, Strano M, Shr S G. In: Siggert K ed, Inter Conf on Hydroforming, Fellbach Germany,2001; 11:363 [4] Xing H L, Makinouchi A. Int J Mech Sci, 2001; 43:1009 [5] Yuan S J, Wang X S, Liu G, Lang L H, Li H Y, Wang Z R. Processing of the 7th ICTP. Yokohama, Japan: Japan Society for Technology of Plasticity, 2002:14952 |
|