| NiAl微晶涂层对两种NiAl基共晶合金高温氧化性能的影响 |
| 徐春梅 郭建亭 |
| 中国科学院金属研究所;沈阳110016 |
|
引用本文:
徐春梅; 郭建亭 . NiAl微晶涂层对两种NiAl基共晶合金高温氧化性能的影响[J]. 金属学报, 2002, 38(7): 673-678 .
[1] Darolia R. JOM, 1991; 43:44 [2] Miracle D B. Acta Metall Mater, 1993; 41: 649 [3] Bowman R R, Misra A K, Arnold S M. Metall Trans,1995; 26A: 615 [4] Liu C Y, Jeng S M, Yang J M, Amato R A. Sci Eng, 1995;A191: 49 [5] Johnson D R, Chen X F, Oliver B F, Noebe R D, Whit-tenberger J D. Intermet, 1995; 3: 99 [6] Whittenberger J D, Locci I E, Darolia R, Bowman R R.Mater Sci Eng, 1999; A268: 165 [7] Cui C Y, Guo J T. Acta Metall Sin, 1999; 35: 477(崔传勇,郭建亭.金属学报,1999;35:477) [8] Guo J T, Cui C Y, Chen Y X, Li D X, Ye H Q. Intermet,2001; 9: 287 [9] Qi Y H, Guo J T, Cui C Y. Chin J Mater Res, 2001, 15:209(齐义辉,郭建亭,崔传勇.材料研究学报,2001;15:209) [10] Guo J T, Qi Y H, Cui C Y, Li G S. Proc PRICM4, Editor:Hanada S, 2001; to be published [11] Xu C M, Guo J T, Yang F B. Acta Metall Sin, 2001; 37:857(徐春梅,郭建亭,杨福宝.金属学报,2001;37:857) [12] Xu C M, Guo J T, Yang F B. J Mater Eng, 2001; to bepublished [13] Wang F H, Lou H Y. Mater Sci Eng, 1990; A129: 279 [14] Tang Z L, Wang F H, Wu W T. Oxid Met, 1997; 48: 511 [15] Yang S L, Wang F H. Acta Metall Sin, 2000; 36: 985(杨松岚,王福会.金属学报,2000;36:985) [16] Walkwork G R, Hed A Z. Oxid Met, 1971; 3: 229 [17] Gleeson B, Cheung W H, Young D J. Corros Sci, 1993;35: 923 [18] Prajitno D, Gleeson B, Young D J. Corros Sci, 1997; 39:639 [19] Phillips M A, Gleeson B. Oxid Met, 1998; 50: 399 [20] Whittle D P, Stringer J. Philos Trans R Soc Londen SerA, 1980; 285: 309 [21] Rybicki G C, Smialek J L. Oxid Met, 1989; 31: 275 [22] Brumm M W, Grabke H J. Corros Sci, 1992; 33: 1677^ |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|