| SS400钢焊接接头表层组织纳米均一化及硬度均一化处理 |
| 李东 陈怀宁 刘刚 卢柯 |
| 中国科学院金属研究所;沈阳110016 |
|
引用本文:
李东; 陈怀宁; 刘刚; 卢柯 . SS400钢焊接接头表层组织纳米均一化及硬度均一化处理[J]. 金属学报, 2001, 37(9): 980-984 .
[1] Zhang W Y. Metallurgy of Welding. Beijing: MechanicalIndustry Press, 1997: 188(张文钺 焊接冶金学 北京:机械工业出版社,1997:188) [2] Gleiter H. Prog Mater Sci, 1989; 33: 223 [3] Hughes R O, Smith S D, Pande C S, Johnson H R, Arm-strong R W. Scr Metall, 1986; 20: 93 [4] Li Z G, Smith D J. Appl Phgs Lett, 1989; 55: 919 [5] Inoue A. Mater Sci Eng, 1994; A179: 57 [6] Kear B H, Strutt P R. Nanostrvct Mater, 1995; 6: 227 [7] Birringer R, Gleiter H, Klein H P, Marquardt P. Phys Lett,1984; 102A: 365 [8] Koch C C. Nanostruct Mater, 1997; 9: 13 [9] Lu K. Mater Sci Eng, 1996; R16: 161 [10] Erb U, El-Sherik A M, Palumbo G, Aust K T. NanostrucMater, 1993; 2: 383 [11] Lu K, Lu J. J Mater Scl Technol, 1999; 15: 193 [12] Tao N R, Sui M L, Lu J, Lu K. Nanostruct Mater, 1999;11: 433 [13] Liu G, Lu J, Lu K. Mater Sci Eng, 2000; A286: 91 [14] Liu G, Wang S C, Lou X F, Lu J, Lu K. Scr Mater, 2001(in print) [15] Altenberger I, Scholtes B, Martin U, Oettel H. Mater SciAng, 1999; 264A: 10 [16] Lu K, Lu J. Chin in Pat, 99122670. 4, 1999 [17] Klug H P, Alexander L E. X-ray Diffraction Proceduresfor Polycrystalline and Amorphous Materials, 2nd Ed-tion, New York: Wiley, 1974: 662 [18] Tian H H, Atzamon M. Acta Mater, 1999; 47: 1255Z |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|