| 原位生成TiC对快凝Al-Fe-V-Si合金中 "块状相"生成的影响 |
| 孙玉峰 张国胜 沈宁福 熊柏青 张永安 |
| 北京科技大学材料学院;北京100083 |
|
引用本文:
孙玉峰; 张国胜; 沈宁福; 熊柏青; 张永安 . 原位生成TiC对快凝Al-Fe-V-Si合金中 "块状相"生成的影响[J]. 金属学报, 2001, 37(11): 1193-1197 .
[1] Guan S K, Shen N F, Tang Y L. Acta Metall Sin, 1996;32: 823(关绍康,沈宁福,汤亚力.金属学报,1996;32:823) [2] Chen L Q, Shen N F, Sun G X. Acta Metall Sin, 1995; 31:295(陈龙庆,沈宁福,孙国雄.金属学报,1995; 31:295) [3] Allen C M, O'Reilly K A Q, Cantor B. Prog Mater Sci,1998; 43: 89 [4] Allen C M, O'reilly K A Q, Evans P V. Acta Mater, 1999;47: 4387 [5] Shen N F, Tang Y L, Guan S K. Acta Metall Sin, 1996;32: 673(沈宁福,汤亚力,关绍康. 金属学报,1996;32:673) [6] Shao G, Tsakiropoulous P, Miodownik A P. Mater SciTechnol, 1997; 13: 1 [7] Shao G, Tsakiropoulous P. Acta Metall Mater, 1994; 42:2937 [8] Tong X C, Shen N F, Fang H S. J Mater Sci, 1995; 30:3680 [9] Tang Y L. Ph D Thesis, Tsinghua University, 1997(汤亚力,博士学位论文,清华大学,1997) [10] Gilgien P, Zryd A, Kurz W. Acta Metall Mater, 1995; 43.3477 [11] Magnin P, Trivedi R. Acta Metall Mater, 1991; 39. 453 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|