| SiC晶须增强6061Al基复合材料的热机械疲劳性能Ⅰ.应力应变行为 |
| 钱立和 王中光 户田裕之 小林俊郎 |
| 中国科学院金属研究所材料疲劳与断裂国家重点实验室;沈阳1100116 |
|
引用本文:
钱立和; 王中光; 户田裕之; 小林俊郎 . SiC晶须增强6061Al基复合材料的热机械疲劳性能Ⅰ.应力应变行为[J]. 金属学报, 2001, 37(11): 1198-1202 .
[1] McDanels D L. Metall Trans, 1985; 16A: 1105 [2] Christman T, Needleman A, Nutt S R, Suresh S. MaterSci Eng, 1989; 107A: 49 [3] Vyletel G M, Allison J E, Van Aken D C. Metall MaterTrans, 1995; 26A: 3155 [4] Han N L, Wang Z G, Su L Z. Scr Metall Mater, 1995; 32:1739 [5] Sehitoglu H. J Eng Mater Technol, 1985; 107: 221 [6] Mall S, Schubbe J J. Com Sci Technol, 1994; 50: 49 [7] Gabb T P, Gayda J, Mackay R A. J Com Mater, 1990;24: 667 [8] Revelos W C, Jones J W, Dolley E J. Metall Mater Trans,1995; 26A: 1167 [9] Sehitoglu H, Karayaha M. In: Kitaue H, Tanaka T eds,Proc of the 4th International Conference on Fatigue andFatigue Thresholds, Honolulu Hawaii, 1990: 1693 [10] Lee E U. Metall Mater Trans, 1994; 25: 2207 [11] Toda H, Kobayashi T, Niinomi M. J Japan Inst Metals,1994; 58: 468 [12] Engler-Pinto Jr C C, Rezai-Aria F. Fatigue'96 Paris,1996: 831 [13] Chrisman T, Suresh S. Acta Metall, 1988; 36: 1691 [14] Vogelsang M, Arsenault R J, Fisher R M. Metall Trans,1986; 17A: 379 [15] Zauter R, Petry F H, Christ J, Mughrabi H. In: SehitogluH ed. Thermo-mechanical Fatigue Behavior of Materials,Philadephia: American Society for Testing and Materials,ASTM STP 1186. 1993: 70 [16] Qian L H, Wang Z G, Toda M, Kobyashi T. Acta MetallSin. 2001; 37: 1203(钱立和.王中光,户田裕之,小林俊郎.金属学报,2001;37:1203)w |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|