| 激光熔覆大厚度Fe57Co8Ni8Zr10Si4B13非晶表层及其微结构研究 |
| 武晓雷 洪友士 |
| 中国科学院力学研究所非线性力学国家重点实验室;北京 100080 |
|
引用本文:
武晓雷; 洪友士 . 激光熔覆大厚度Fe57Co8Ni8Zr10Si4B13非晶表层及其微结构研究[J]. 金属学报, 2000, 36(12): 1244-1247 .
[1] Cahn R W. Nature, 1976; 260: 285 [2] von Allmen M. Top Appl Phys, 1983; 53: 261 [3] Wu X L, Hong Y S. Trans Met Heat Treat, 2000; 21: inpress(武晓雷,洪友士.金属热处理学报,2000;21:待发表) [4] Morris D G. Mater Sci Eng, 1988; 97A: 177 [5] Wang W K, Lobb C J, Spaepen F. Mater Sci Eng, 1988;98A: 325 [6] Hirose F, Takagi M, Mori H, Kitoh Y, Imura T. Jpn JAppI Phys, 1992; 31: 3940 [7] Inoue A. Mater Trans JIM, 1995; 36: 866 [8] Johnson W L. Mater Sci Forum, 1996; 35: 225 [9] Inoue A, Gook J S. Mater Trans JIM, 1996; 37: 32 [10] Inoue A, Zhang T, Itoi T, Takeuchi A. Mater Trans JIM,1997; 38: 359 [11] Inoue A, Miyauchi Y, Makino A, Masumoto T. MaterTrans JIM, 1996; 37: 78 [12] Wang W H, Wei Q, Friedrich S, Macht M P, Wanderka N,Wollenberger H. Appl Phys Lett, 1997; 71: 1053 [13] Wang W H, Wang W K, Bai H Y. Sci Chin, 1998; 28A:443(汪卫华,王文魁,白海洋.中国科学,1998;28A:443) [14] He G, Bian Z, Chen G L. Mater Sci Eng, 2000; 279A: 237 [15] He G, Bian Z, Chen G L. Acta Metall Sin, 1999; 35: 458(何国,边赞,陈国良.金属学报,1999;35:458) [16] Greer A L. Nature, 1993; 366: 303 [17] Illekova E, Jergel M, Dubai P, Inoue A. Mater Sci Eng,1997; 226-228A: 388/ |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|