| Zr52.5Ni14.6Al10Cu17.9Ti5块体玻璃合金等温晶化与结构转变 |
| 何国 边赞 陈国良 |
| 北京科技大学金属材料国家重点实验室; 北京 100083 |
|
引用本文:
何国; 边赞; 陈国良 . Zr52.5Ni14.6Al10Cu17.9Ti5块体玻璃合金等温晶化与结构转变[J]. 金属学报, 1999, 35(5): 458-462 .
[1] Inoue A. Mater Tabes JIM, 1995; 36: 866 [2] Peker A, Johnson L. Appl phes Lett, 1993; 63: 2342 [3] Singh R N, March N H. In: West brook J H, Fleischer RL eds, Internmentallic Compounds, John Wiley & Sons Ltd,1994: 661 [4] He G, Bian Z, Chen G. Trans Non-ferrous Met Soc China,1999; (9): in press [5] He G, Chen G L. Mated Set Tech, 1998, 6: 105(何国,陈国良.材料科学与工艺,1998;6:105) [6] Illekova E, Jergel M, Dubai P, Inoue K. Mater Set Egg, 1997;226-228A:388 [7] Greer A L. In: West brook J H, Fleischer R L eds, Inter-metallic Compounds, John Wiley & So us Ltd, 1994: 731 [8] Matsubara E, Waseda Y. Mater Trans JIM, 1995, 36: 883 [9] Ostwald W. Phes Chad, 1897, 22. 289 [10] Lu K. Acta Metall Sin, 1994; 30B: 1(卢柯.金属学报, 1994; 30B: 1) [11]Fine M E. Phase Transformation in Condensed System. NewYork:Mac Millan, 1964:1 [12] Thompson C V, Greer A L, Drehman A J. In: Masumoto T,Suzuki K eds, Proc Jib nit Coo f Rapidly Quenched Matals,Sendal: Jpn lust Metals, 1982: 100 [13] Lu K. Ph D Thesis, lust Metal Res, The Chinese Academyof Science, 1989(卢柯.中国科学院金属研究所博士学位论文,1989) [14] Lu K, Wang J T, Dong L. Acta Metall Sin, 1991; 27: B31(卢柯,王景唐,董林.金属学报, 1991; 27B: 31)y |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|