定向凝固NiAl-28Cr-5.5Mo-0.5Hf合金中Ni2AlHf相和Ni16Hf6Si7相的研究 |
陈玉喜 刘志权 贺连龙 崔传勇 李斗星 郭建亭 |
中国科学院金属研究所固体原子像开放研究实验室; 沈阳 110015 |
|
引用本文:
陈玉喜; 刘志权; 贺连龙; 崔传勇; 李斗星; 郭建亭 . 定向凝固NiAl-28Cr-5.5Mo-0.5Hf合金中Ni2AlHf相和Ni16Hf6Si7相的研究[J]. 金属学报, 1999, 35(11): 1151-1154 .
[1] Cline H E, Walter J L. Met Trans, 1970; 1: 2907 [2] Cline H E, Walter J L, Lifshin E, Russell R R. Met Trans,1971; 2: 189 [3] Yang J M, Jeng S M, Bain K, Amato R A. Acta Metall, 1997;45: 295 [4] Darolia R. JOM, 1991; 43(3):44 [5] Chen Y X, Cul C Y, He L L, Guo J T, Li D X. Acta MetallSin, 1999; 35(Suppl.2):444(陈玉喜,崔传勇,贺连龙,郭建亭,李斗星.金属学报,1999;35(增刊2):444) [6] Locci I E, Dickerson RM, Garg A, Noebe R D, Whittenbetger J D, Nathal M V, Darolia R J. Mater Res, 1996; 11:3024 [7] Garg A, Noebe R D, Darolia R. Acta Metall, 1996; 44: 2809 [8] Lu P, Cosandey F. Acta Metall, 1992; 540: 259 [9] Li D X, Pirouz P, Hener A H, Yadavalli S, Flynn C P. PhilMag, 1992; A65: 403 [10] Jesser W A, Kuhlmann-Wilsdorf D. Phys Status Solidi,1967;31: 533. [11] Wen S H, Kostlan E, Hong M, Khachaturyan A G, Morris JW Jr. Acta Metall, 1981, 29. 1247 [12] Wasilewski R J. Trans TMS-AIME, 1966; 236: 455 [13] Locci. I.E, Noebe R D, Bowman R R, Miner R V, Nathal MV, Darolia R. Mater Res Soc Symp Proc, 1991; 213: 1013 [14] Takeyama M, Liu C T. J Mater Res, 1989; 5: 1189> |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|