Please wait a minute...
金属学报  1999, Vol. 35 Issue (10): 1009-1020     
  论文 本期目录 | 过刊浏览 |
晶界非平衡偏聚研究的回顾与展望
吴平 贺信莱
北京科技大学材料物理系; 北京 100083
引用本文:

吴平; 贺信莱 . 晶界非平衡偏聚研究的回顾与展望[J]. 金属学报, 1999, 35(10): 1009-1020 .

全文: PDF(1188 KB)  
摘要: 面结构及运动均有重要影响. 本文综述了连续冷却与高速淬火等温过程静止晶界上溶质非平衡偏聚研究已获得的主要实验规律, 分析评述了已有的主要理论模型, 讨论了当前存在的问题. 同时还评述了近年来移动界面溶质反常偏聚研究的实验研究和理论研究现状.
关键词 : 合金,  溶质,  晶界,  非平衡偏聚    
Key words:
收稿日期: 1999-06-22     
ZTFLH:  TG111.2  
[1] Lea C, Seah M P. Philos Mag, 1977; 35: 213
[2] Guttman M. Philos frans R Soc, 1980; A295: 169
[3] Tipler H R, Hopkins B E. Met Sci, 1976; 10: 47
[4] Yu J, Grabke H J. Met Sci, 1983; 17: 389
[5] Seah M P. Philos Trans R Soc, 1980; A295: 265
[6] Bandhopadhyay N, Briant C L. Metall Trans, 1983; 14A:2005
[7] Hondros E D, Seah M P, Lea C. Metals Mater, 1976; Jan-uary: 26
[8] Buretein G T, Woodword J. Met Sci, 1983; 17: 11
[9] Bandhopadhyay N, Briant C L. Corrosion, 1982; 38: 125
[10] McMohan C J. Mater Sci Eng, 1980; 42: 215
[11] Hondros E D, Seah M P. Int Metall Rev, 1977; 22: 262
[12] Misra R D K, Rasad C Y, Balasubramanian T V, Rao P R.Scr Metall, 1986; 20: 713
[13] Seah M P. J Phys F: Metal Phys, 1980; 10: 1043
[14] He X L, Chu Y Y, Zhang X L, Yu Z S. Acta Metall Sin,1977; 13: 235(贺信莱,褚幼义,张秀林,余宗林,金属学报,1977;13:235)
[15] Mclean D. Gruin Boundaries in Metals. London: OxfordUniversity Press, 1957: 118
[16] Guttmann M. Surf Sci, 1975; 53: 213
[17] Karlsson L, Norden H, Odelius H. Acta Metall, 1988; 36: 1
[18] KarI8s0n L, Norden H, Odelius H. Acta Metall, 1988; 36: 13
[19] Williams T W, Stoneham A M, Harries D R. Met Sci, 1976;10: 14
[20] Williams T W. Atomic Enerpy Researeh Establishment. Har-well: Berks, 1972: 68
[21] Keown S R, Pickering F B. Met Sci, 1977; 7: 225
[22] He X L, Chu Y Y, Ko T. Acta Metall Sin, 1982; 18: 1(贺信莱,褚幼义,柯俊,金属学报,1982; 18: 1)
[23] He X L, Chu Y Y, Jonas J J. Acta Metall, 1989; 37: 147
[241 He X L, Chu Y Y, Jonas J J. Acta Metall, 1989; 37: 2905
[25] He X L, Chu Y Y. J Phys D: Appl Phys, 1983; 16: 1145
[26] He X L, Chu Y Y. J Beijing Iron Steel Inst, 1981; 2: 99(贺信莱,褚幼义,北京钢铁学院学报,1981; 2: 99)
[27] Karlsson L, Norden H. J Physique, 1984; C9: 391
[28] Karlsson L, Andren H O, Norden H. Scr Metall, 1982; 16:297
[29] He X L, Chu Y Y. Phys Chem Anal: Phys, 1979; (6): 25(贺信莱,褚幼义,理化检验(物理分册),1979; (6): 25)
[30] He X L, Chu Y Y. Phys Chem Anal: Phys, 1979; (5): 29(贺信莱,褚幼义,理化检验,(物理分册), 1979; (5): 29)
[31] He X L, Chu Y Y, Ke J. Acta Metall Sin, 1983; 19: A459(贺信莱,褚幼义,柯俊,金属学报,1983; 19: A459)
[32] Yoshida M. Scr Metall, 1982; 16: 787
[33] Karlsson L, Norden H, Odelius H. Acta Metall, 1988; 36: 35
[34] Doig P, Plewitt P E J. Metall frans, 1987; 18A: 399
[35] 孙大涌,锰低温钢奥氏体界面元素不平衡偏聚及其脆断机制的研 究,国家自然科学基金项目(No.59341009)报告,1997
[36] Faulkner R G, Hopkins T C, Norroard K. X-ray Spectrom-etry, 1977; 6: 73
[37] Vorlicek V, Flewitt P E. J. Acta Metall Mater, 1994; 42:3309
[38] Doig P, Plewitt P E J. Acta Metall, 1981; 29: 1831
[39] Misra R D K, Balasubramanian T V, Rao P R. Acta Metall,1987; 35: 2995
[40] Misra R D K, Rao P R. Mater Sci Technol, 1997; 13: 277
[41] He X L, Chu Y Y, Tang L, Zhou Z X, Ke J. Acta Metall Sin,1987; 23: A291(贺信莱,褚幼义,唐立,周振新,柯俊,金属学报, 1987;23: A291)
[42] Huang X, Chaturvedi M C, Richards N L, Jackman J. ActaMater, 1997; 45: 3095
[43l He X L, Chu Y Y, Yu Z S, Ou Y F. Acta Metall Sin, 1980;16: 380(贺信莱,褚幼义,余宗森,欧宇夫,金属学报,1980; 16: 380)
[44] Chu Y Y, He X L, Tang L, Xu T D, Ke J. Acta Metall Sin,1987; 23: A169(贺幼义,贺信莱,唐立,徐庭栋,柯俊,金属学报,1987;23: A169)
[45] Chu Y Y, He X L, Ko T. Mater Sci Progr, 1988; 2: 18(褚幼义,贺信莱,柯俊,材料科学进展, 1988; 2: 18)
[46] Willams D B, Romig A D Jr. Utramicroscopy, 1989; 30: 38
[47] Erb U, Aust K T. Scr Metall, 1984; 18: 1263
[48] Misra P D K. Scr Metall, 1985; 19: 1177
[49] Joshi A. Metall Trans, 1981; A12: 1081
[50] Chen N, Yu Z S. J Univ Sci Technol Beijing, 1992; 14: 577(陈宁,余宗森,北京科技大学学报,1992; 14: 577)
[51] Bercovici S J, Hunt C E L, Niessen P. J Mater Sci, 1970; 5:326
[52] Faulkner R G. J Mater Sci, 1981; 16: 373
V[53] Letellier L, Guttmann M, Blavette D. Phllos Mag Lett, 1994;70: 189
[54] Muschik T, Gust W, Hofmann S, Predel B. Acta Metall,1989; 37: 2917
[55] Westbrook J H, Aust K T. Acta Metall, 1963; 11: 1151
[56] Aust K T, Peat A J, Westbrook J H. In: Cotterill R M J ed,Lattice Defects ln Quenched Metals, New York: AcademicPress, 1965: 771
[57] Aust K T, Hanneman R E, Niessen P J, Westbrook J H. ActaMetall, 1968; 16: 291
[58] Aust K T, Peat A J, Westbrook J H. Acta Metall, 1966; 14:1469
[59] He X L, Chu Y Y, Ke J, Acta Metall Sin, l982; 18: 12(贺信莱,褚幼义,柯俊,金属学报,1982; 18: 12)
[60] Hanneman R E, Anthony T R. Acta Metall, 1969; 17: 1133
[61] Cui H Y. PhD Dissertatton, University of Science and Tech-nology Beijing, 1996(崔怀洋,北京科技大学博士学位论文,1996)
[62] Cui H Y, He X L. Acta Metall Sin, 1999; 35: 239(崔怀洋,贺信莱,金属学报,1999; 35: 239)
[63] Heo N H. Acta Mater, 1996; 44: 1581
[64] Heo N H. Acta Mater, 1996; 44: 3015
[65] Heo N H, Lee H C. Metall Mater Trans, 1996; 27A: 1O15
[66] Heo N H. Metall Mater fons, 1996; 27A: 3059
[67] for P R. Res Account, 1997; 73: 580
[68] Dumoulin P, Guttman M. Mater Sci Eng, 1981; 42: 249
[69] Anthony T R. Acta Metall, 1969; 17: 603
[70] Xu T D. J Mater Sci, 1987; 22: 337
[71] Xu T D. J Mater Sci Lett, 1988; 7: 241
[72] Song S H, Xu T D, Yuan Z X. Acta Metall, 1989; 37: 319
[73] Chapman M A V, Faulkner R G. Acta Metall, 1983: 31: 677
[74] Karlsson L, Norden H, 0delius H. Acta Metall, 1988; 36: 25
[75] Chu Y Y, Zhang S H, He X L, Ke J. Acta Metall Sin, 1989;25: A275(褚幼义,章三红,贺信莱,柯俊,金属学报,1989; 25: A275)
[76] Zhang S H, He X L, Chu Y Y, Ke J. Acta Metall Sin, 1992;28: A187(章三红,贺信莱,褚幼义,柯俊,金属学报, 1992; 28: A187)
[77] Zhang S H, He X L, Ko T. J Mater Sci, 1994; 29: 2663
[78] Faulkner R G, Jiang H. Mater Scl Technol, 1993; 9: 665
[79] Jiang H, Faulkner R G. Acta Mater, 1996; 44: 1857
[80] Song S H, Xu T D. J Mater Sci, 1994; 29: 61
[81] Carolan R A, Faulkner R G. Acta Metall, 1988; 36: 257
[82] Xu T D. In: Gao H ed, Ultra High Strength and DuctileSteel, Beijing: Editoria1 Staff of” J Iron Steel Res”, 1998:22(徐庭栋,见:高 怀主编,高强高韧钢文集,北京:《钢铁研究学报》编辑部,1998: 22)
[83] Xu T D, Song S H, Shi H Z, W.Gust, Yuan Z X. Acta MetallMater, 1991; 39: 3119
[84] Wang W D, Zhang S H, He X L. Acta Metall Mater, 1995;43: 1693
[85] Mega T, Shimomura J, Yasuhara E, Mater frans JIM, 1995;36: 1206
[86] Kasen M B. Acta Metall, 1972; 20: 106
[87] Kassen M B. Acta Metall, 1983; 31: 489
[88] Barbier-Vitart J, Saindrenan G. J Mater Sci, 1982: 17: 387
[89] Saindrenan G, Larere A. Scr Metall, 1984; 18: 969
[90] Cui H Y, He X L, Ke J. Mater Sci Eng, 1995; 13: 2(崔怀洋,贺信莱,柯俊,材料科学与工程,1995; 13: 2)
[91] Cao B, He X L. J Univ Sci Technol Beijing, 1998; 20: 266(曹兵,贺信莱,北京科技大学学报,1998; 20: 266)
[92] He X L, Djahazi M, Jonas J J, Jackman J. Acta MetallMater, 1991; 39: 2295
[93] Zhang S H, He X L, Ke J. J Univ Sci Technol Beijing, 1992;14: 364(章三红,贺信莱,柯俊,北京科技大学学报,1992; 14: 364)
[94] Zhang S H, He X L, Ko T. Scr Metall Mater 1992; 26: 567
[95] Zhang S H, He X L, Chu Y Y, Ko T. J. Mater Sci, 1994; 29:2655
[96] Tan D L, He X L, Yu Z S. i Iron Steel Res, 1997; 9: 34(谭佃龙,贺信莱,余宗森,钢铁研究学报,1997; 9: 34)
[97] Yang S W. PhD Dissertation, University of Science and Tech-nology Beijing, 199(杨善武,北京科技大学博士学位论文,1997)
[98] Simpson C J, Aust K T, Winegerd W C. Metall frans, 1970;1: 1482
[99] Cahn J W. Acta Metall, 1962; 10: 789
[100] Lucke K, Stuwe H P. In: Himmel L ed., Recovery and Re-crystallization of Metals. New York: Interscience, 1963: 171
[101] Zhang S H. PhD Dissertation, University of Science andTechnology Beijing, 1991(章三红,北京科技大学博士学位论文,1991)
[1] 杜金辉, 毕中南, 曲敬龙. 三联冶炼GH4169合金研究进展[J]. 金属学报, 2023, 59(9): 1159-1172.
[2] 李嘉荣, 董建民, 韩梅, 刘世忠. 吹砂对DD6单晶高温合金表面完整性和高周疲劳强度的影响[J]. 金属学报, 2023, 59(9): 1201-1208.
[3] 白佳铭, 刘建涛, 贾建, 张义文. 高W高Ta型粉末高温合金的蠕变性能及溶质原子偏聚[J]. 金属学报, 2023, 59(9): 1230-1242.
[4] 江河, 佴启亮, 徐超, 赵晓, 姚志浩, 董建新. 镍基高温合金疲劳裂纹急速扩展敏感温度及成因[J]. 金属学报, 2023, 59(9): 1190-1200.
[5] 王磊, 刘梦雅, 刘杨, 宋秀, 孟凡强. 镍基高温合金表面冲击强化机制及应用研究进展[J]. 金属学报, 2023, 59(9): 1173-1189.
[6] 毕中南, 秦海龙, 刘沛, 史松宜, 谢锦丽, 张继. 高温合金锻件残余应力量化表征及控制技术研究进展[J]. 金属学报, 2023, 59(9): 1144-1158.
[7] 郑亮, 张强, 李周, 张国庆. 增/降氧过程对高温合金粉末表面特性和合金性能的影响:粉末存储到脱气处理[J]. 金属学报, 2023, 59(9): 1265-1278.
[8] 马德新, 赵运兴, 徐维台, 王富. 重力对高温合金定向凝固组织的影响[J]. 金属学报, 2023, 59(9): 1279-1290.
[9] 陈佳, 郭敏, 杨敏, 刘林, 张军. 新型钴基高温合金中W元素对蠕变组织和性能的影响[J]. 金属学报, 2023, 59(9): 1209-1220.
[10] 卢楠楠, 郭以沫, 杨树林, 梁静静, 周亦胄, 孙晓峰, 李金国. 激光增材修复单晶高温合金的热裂纹形成机制[J]. 金属学报, 2023, 59(9): 1243-1252.
[11] 宫声凯, 刘原, 耿粒伦, 茹毅, 赵文月, 裴延玲, 李树索. 涂层/高温合金界面行为及调控研究进展[J]. 金属学报, 2023, 59(9): 1097-1108.
[12] 赵鹏, 谢光, 段慧超, 张健, 杜奎. 两种高代次镍基单晶高温合金热机械疲劳中的再结晶行为[J]. 金属学报, 2023, 59(9): 1221-1229.
[13] 冯强, 路松, 李文道, 张晓瑞, 李龙飞, 邹敏, 庄晓黎. γ' 相强化钴基高温合金成分设计与蠕变机理研究进展[J]. 金属学报, 2023, 59(9): 1125-1143.
[14] 张健, 王莉, 谢光, 王栋, 申健, 卢玉章, 黄亚奇, 李亚微. 镍基单晶高温合金的研发进展[J]. 金属学报, 2023, 59(9): 1109-1124.
[15] 张海峰, 闫海乐, 方烽, 贾楠. FeMnCoCrNi高熵合金双晶微柱变形机制的分子动力学模拟[J]. 金属学报, 2023, 59(8): 1051-1064.