| 铝基复合材料中颗粒在凝固界面的行为 |
| 吴树森;中江秀雄 |
| 华中理工大学材料科学与工程系;武汉;430074;日本早稻田大学 |
|
| BEHAVIOR OF PARTICLES AT SOLIDIFICATION INTERFACE OF ALUMINUM MATRIX COMPOSITES |
| WU Shusen (Department of Materials Science and Engineering; Huazhong University of Science and Technology; Wuhan 430074)NAKAE Hideo Waseda Univeristy; Tokyo; Japan Correspondent: WU Shusen; associate professor Tel: (027)87543876(O); (027)87547469(H);Fax: (027)87548737 |
引用本文:
吴树森;中江秀雄. 铝基复合材料中颗粒在凝固界面的行为[J]. 金属学报, 1998, 34(9): 939-944.
,
.
BEHAVIOR OF PARTICLES AT SOLIDIFICATION INTERFACE OF ALUMINUM MATRIX COMPOSITES[J]. Acta Metall Sin, 1998, 34(9): 939-944.
1 Rohatgi P K, YarandiF M, Liu Y, Asthana R. Mate, Sci Eng, 1991; A147(3): L1 2 MeNelleyard T R, Kalu P N. Scr Metall Mater, 1991; 25: 1041 3 吴树森,中江秀雄.铸造工学,1997;69:775(Wu S, Nakae H.J JpnFoundry Eng Soc, 1997, 69: 775) 4 吴树森.日本早稻田大学博士论文,1997(Wu S S, PhD thesis, Waseda University Tokyo, 1997) 5 吴树森,中江秀雄.铸造工学,19972 69:3(Wu S, Nakae H. J Jpn Foundry Eng Soc,1997; 60: 3) 6 Nakae H, Wu S. Key Eng Mater , 1997 127: 503 7 NakaeH, Fujii H, Shinohara T, Zhao B R. Proc. ICCM/9; 1993: 559 8 Omenyi S N, Neumann A W.J Appl phys, 1976, 47: 3956 9 长隆郎,冲猛雄.日本金属学会志,1987;51:1209(Choh T,Oki T.J Jpn Inst Met,1987;51:1209) 10 Nakae H,Wu S.Proc Fifth Asian FoundryCong,1997:408 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|