| Ag-Cu共晶合金在落管中的快速凝固 |
| 王楠;曹崇德;魏炳波 |
| 西北工业大学应用物理系;西安;710072;西北工业大学应用物理系;西安;710072;西北工业大学应用物理系;西安;710072 |
|
| RAPID SOLIDIFICATION OF Ag-Cu EUTECTIC ALLOY BY DROP TUBE PROCESSING |
| WANG Nan; CAO Chongde; WEI Bingbo(Department of Applied Physics; Northwestern Polytechnical University; Xi'an 710072)Correspondent. WANG Nan; Doctoral candidate; Tel: (029)8493350; Fax: (029)8492074 |
引用本文:
王楠;曹崇德;魏炳波. Ag-Cu共晶合金在落管中的快速凝固[J]. 金属学报, 1998, 34(8): 824-830.
,
,
.
RAPID SOLIDIFICATION OF Ag-Cu EUTECTIC ALLOY BY DROP TUBE PROCESSING[J]. Acta Metall Sin, 1998, 34(8): 824-830.
1 Murarka R, Lu W-K, Hamielec A E. Metall Trans, 1971; 2: 2949 2 Walder S, Ryder P L. J Appl Phys, 1993; 74: 6100 3 Parsad Y V S S, Ramachandra Rao P, Chattopadhyay K. Acta Metall, 1984; 32: 1825 4 Wei B, Yang G, Zhou Y. Hangkong Xueboo. 1990; 11: A59 5 Wei B, Herlach D M, Feuerbacher B, So mmer F. Acta Metall Maten 1993; 41: 1801 6 Greer A L. Mater Sci Eng, 1994; A178: 113 7 Jackson K A, Hunt J D. Trans Met Soc AIME 1966; 236: 1129 8 Thivedi R, Magnin P, Kurz W. Acta Metall, 1987; 35: 971 9 Beck D G, Copley S M, Bass M. Metall Trans, 1981; 12A: 1687 10 Boswell P G, Chadwick G A. J Mat Sci, 1977; 12: 1879 11 Boettinger W J. In: Kear B H, Giessen B C, Cohen M eds., Mater Res Soc Symp Proc, New York: Elsevier Science Pubishing Co, 1982; 8: 15B |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|