| 准下贝氏体的孪晶及形成机制 |
| 栾道成;魏成富;杨哿 |
| 四川工业学院材料科学与工程系;成都;611744;四川工业学院材料科学与工程系;成都;611744;四川工业学院材料科学与工程系;成都;611744 |
|
| TWINS AND ITS FORMATION MECHANISM IN LOWER META-BAINITE |
| LUAN Daocheng; WEI Chengfu;YANG Ge (Department of Materials Science and Engineering; Sichuan Institute of Technology; Chengdu 611744) |
引用本文:
栾道成;魏成富;杨哿. 准下贝氏体的孪晶及形成机制[J]. 金属学报, 1998, 34(1): 24-30.
,
,
.
TWINS AND ITS FORMATION MECHANISM IN LOWER META-BAINITE[J]. Acta Metall Sin, 1998, 34(1): 24-30.
1 Sandvik B P J, Metall Trans, 1982 13A: 777 2 Kang M K,Sun J L,Yang Q M.Metall Trzns,1990; 21A: 853 3 Huang D H,Thomas G Metall Trans,1977;8A:1661 4 张喜燕,康沫狂,陈大明,武小雷.金属学报,1994;30:A109(Zhang Xiyan.Kang Mokuang,Chen Daming,Wu Xiaolei.Acta Metall Sin,1994:30:A109) 5 康沫狂,杨延清,张喜燕.孙加林,贾虎生,武小雷金属学报,1996;32:A897(Kang Mokuang, Yang Yanqing; Zhang Xlvan, Sun Jialin; Jia Husheng,Wu Xiaolei. Acta Metall Sin,1996, 22:897) 6 Okamoto H, Oka M,Metall Trans, 1986;17A:1113 7 杨立波,刘文西,陈玉如,龚方岳,陈金铭钢铁,1989;24(9):43(Yang Libo;Liu Wenxi,Chen Yuru,Gong Fangyue,Chen Jinming.Iron Steel, 1989; 24(9): 43) 8 孙加林,康沫狂。西北工业大学学报, 1990;(SuPPl): 73(Sun Jialin,Kang Mokuang.J Northwestern Poly Uni,1990;(Suppl):73) 9 栾道成,魏成富,杨哿.钢铁研究学报,1996;8(6):24(Luan Daocheng, Wei Chengfu; Yang Ge.J Iron Steel Res,1996 8(6): 24) 10 Sandvik B P J,Wayman C M Metall Trans,1983 14A: 823 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|