固体范性形变与断裂的介观力学物理原理(英文)
V.E.Panin
TheInstituteofStrengthPhysicsandMaterialsSciences;RussianAcademyofSciences;SiberianBranch;Tomsk;634048;Russia
PHYSICAL FUNDAMENTALS OF MESOMECHANICS OF PLASTIC DEFORMATION AND FRACTURE OF SOLIDS
V.E.Panin(The Institute of Strength Physics and Materials Sciences; Russian Academy of Sciences;Siberian Branch; Tomsk; 634048; Russia)
引用本文:

V.E.Panin. 固体范性形变与断裂的介观力学物理原理(英文)[J]. 金属学报, 1997, 33(2): 187-197.
. PHYSICAL FUNDAMENTALS OF MESOMECHANICS OF PLASTIC DEFORMATION AND FRACTURE OF SOLIDS[J]. Acta Metall Sin, 1997, 33(2): 187-197.

全文: PDF(4379 KB)  
摘要: 本文回顾了建立在物理介视力学基础上的固体范性形变与断裂的研究概况,从物理介现力学角度看,处于载荷下的固体是一个多层次的自治体系.依尺度不变原理,在微观、介观、宏观尺度上的范性流变,本质上是相互关联的.整体介观体积在介观尺度上按照“切变加旋转”的方式运动.固体范性形变与断裂可考虑为同样过程的二个阶段.
关键词 : 介观力学,  范性形变,  断裂    
Abstract:The research review on plastic deformation and fracture of solids based on phvsicalmesomechanics is presented. A solid under loading is considered in physicalmesomechanics as multilevel self-consistent system. where the plastic flows atmicro-meso- and macrolevels are natrually interrelated according to the principle ofscaIe invarlance.Bulk mesovolumes are moved at the mesoscale level according toscheme "shear+rotation". Plastic deformation and fracture of solids are considered astwo stages of the same process.
Key words: mesomechanics    plastic deformation    fracturel
收稿日期: 1997-02-18     
1 V.E.Panin, Y.V.Grinyaev, T.F.Elsukova and A.G.Ivanchin, Izv. VUZOV Fisika (6) (1982) 5.
2 V.E.Panin, V.A.Likhachev and Y.V.Grinyaev, Deformation Structural Levels of Solids. (Nauka,Novosibirsk, 1985) p.229.
3 V.E.Panin. V.E.Egorushkin, Yu.A. Chon and T.F.Elsukova, Izv. VUZOP Fisika (12) (1989) 5.
4 Y.V.Grinyaev and N.V.Chertova, Izv. VUZOV. FisikQ (2) (1990) 36.
5 V.E.Panin, Izv. SO AN USSR. Ser. Techn. Sciences 3 (1987) 87.
6 V.E.Panin, Y.V.Grinyaev, V.I.Danilov et al., Structural Levels of Plastic Dekrmation and of Fracture(Nauka, Novosibirsk, 1990) p.225.
7 V.E.Panin, T.F.Elsukova, E.N.Novoselova and V.E.Egorushkin, DAN USSR 310 (l99O) 78.
8 V.E.Egorushkin, Izv. VUZOV. Fizika (4) (1992) 19
9 V.E.Panin and T.F.Elsukova, Synergrtics and FaIikue Fracture of Metals, ed. V. Ivanova (Nauka,Moscow, 1989) p.248.
10 V.E.Panin, Y.V.Grinyaev, V.E.Egorushkin et al., Izv. VUZO V. Fizika (1) (1987) 36.
11 V.E.Panin, T.F.Elsukova, M.K.Eliseeva and Yu.V. Griniaev, Surkce Physics, Chemistry, Mechanics5 (1983) 138.
12 Yu.V.Grinjaev, V.E.Panin, Izv. VUZOV. Ficika (8) (1978) 95.
13 V.E.Panin, Yu.V.Grinyaev et al., DAN USSR 309 (1989) 356
14 V.E.Panin, Izv. VUZOV Ficika (4) (1992) 5.
15 T.F.Elsukova and V.E.Panin, Metals, 2 (1992) 73
16 V.E.Panin, Izv. VUZOV. FisIka (2) (1990) 4.
17 V.E.Panin and K.V.Frolov, The New Physical and Mechanical Methods of Investigation of Materials un-der Loading, ed. V.E.Panin (Tomsk University Press, Tomsk, 1990) p.332.
18 P.V.Makarov, The New Physical and Mechanical Methods of Invesigation of Materials under Loading,ed. V.E.Panin (Tomsk University Press, Tomsk, 1990) p.332.
19 V.E.Panin, Abstracts ofthe frst European East-West Symp. on Materials and Processes (Helsinki1990).
20 V.E.Panin and S.P.Efimenko, Abstracts of the 2nd European Con.f o.f Advanced Materials andProcesses (London, 1991 ) p.288.
21 V.E.Panin, V.E.Egorushkin, T.F.Elsukova and O.V.Veselova, DAN USSR 316 (1990) 1130
22 V.E.Panin, V.E.Egorushkin, T.F.Elsukova and O.V.Veselova, The New Physical and Mechanical Meth-ods ofInvestbotion of MaterJbls under Lnading, ed. V.E.Panin (Tomsk University Press, Tomsk, 1990)P.332.
23 V.E.Panin, T.F.Elsukova, E.M.NovoseIova and V.E.Egorushkin, DAN USSR 276 (1989) 630.
24 K.P.Zhukova, T.F.Elsukova, V.E.Panin and Y.N.Rudenko, Izv. VUZO V. Fisika (4) (1988) 13.
25 V.E.Panin, T.F.Elsukova, E.M.Novoselova and V.E.Egorushikin, DAN USSR 310 (1990) 78.
26 V.E.Panin, L.B.Zuev, V.I.DaniIov and N.M.Mnikh, FMM 66 (1988) 1005.
27 V.E.Panin, L.B.Zuev, V.I.Danilov and N.M.Mnikh, DAN USSR 308 (1989) 1375.
28 V.E.Panin, L.B.Zuev, V.I.Danilov and N.M.Mnikh, FMM 6 (1990) 189.
29 L.B.Zuev, V.E.Panin, V.I.Danilov, N.M.Mnikh and N.V.Peker, DAN USSR 317 (1991) 1386.
30 V.I.Danilov, L.B.Zuev, N.M.Mnikh, V.E.Panin and L.V.Shershova, FMM 3 (1991) 188.
31 V.E.Panin, L.B.Zuev, V.I.Danilov, P.V.Makarov, V.E.Egorushkin, B.B.Gorbatenko, Y.Hida andS.Yoshida, Method and Apporatus for Nondestructive Testing of the Mechanical Behavior ofSolid StateObkct under Loading, RUS Patent, N93002731, Moscow, Russia.
32 V.E.Panin, Y.I.Meshcheryakov, T.F.Elsukova, A.K.Dyvakov, S.G.Psakhie and N.M.Myshlyaev, I:v.VUZO V. Fizka (2) (1990) 107.
33 V.E.Panin, PhySical Mesomechanics and Computer Aided Design of Materials, (Nauku SO, Novosibirsk.v.l, (1995) p.297 and v.2, (1995) p.320.
34 V.E.Panin, Physical Mesomechanics of heterogeneous Medta and Compoter-Aided DesoignofMaterials (Cambridge Interscience Publishing, Cambridge, 1996) p.450.
35 V.E.Panin, Destw 0fNew Materials and Strengthening (Cambridge Interscience Publishing, Cambridge,1996) p.140.
36 V.E.Panin, Jpe. J. Appl. Phys. 9 (1995) 64.
37 V.E.Panin, A.I.Slosman and N.A.Kolesova, FMM 2 (1996) 82.
38 V.E.Panin and T.F.Elsukova, Doclady RAN 5 (1996) 247,617.
39 V.E.Panin and T.F.Elsukova, Izv. VUZO V. Ficika 39 (6) (1996) 40.
40 V.E.Panin, Izv. VUZOV. Fisika 38 (11) (1995) 6.
41 P.V.Makarov, O.I.Cherepanov and V.N.Demidov- I:v. VUZO V. Ficika 38 (11) (1995) 26.
42 S.G.Psakhie, Ya. Horie, S.Yu. Korostelev, A.Yu. Smolin, A.I.Dmitriev, E.V.Shilko and S.V.Alexeev,Izv. VUZOV Fizika 38 (11) (1995) 58.
43 Yu.A.Chon and V.E.Panin, Sold State Phys. 38 (1996) 1767.
44 V.E.Panin, S.V.Panin and A.I.Mamaev, Doclady RAN 1 (1996) 350.
45 V.E.Panin, The Abstracts of Int. Conf" Mathematical Methods in Phystcs, Mechanics andMesomechanics of Fracture", (1996) P. 135.6
[1] 吴进, 杨杰, 陈浩峰. 纳入残余应力时不同拘束下DMWJ的断裂行为[J]. 金属学报, 2022, 58(7): 956-964.
[2] 谷瑞成, 张健, 张明阳, 刘艳艳, 王绍钢, 焦大, 刘增乾, 张哲峰. 三维互穿结构SiC晶须骨架增强镁基复合材料制备及其力学性能[J]. 金属学报, 2022, 58(7): 857-867.
[3] 彭子超, 刘培元, 王旭青, 罗学军, 刘健, 邹金文. 不同服役条件下FGH96合金的蠕变特征[J]. 金属学报, 2022, 58(5): 673-682.
[4] 赵永好, 毛庆忠. 纳米金属结构材料的韧化[J]. 金属学报, 2022, 58(11): 1385-1398.
[5] 胡晨, 潘帅, 黄明欣. 高强高韧异质结构温轧TWIP钢[J]. 金属学报, 2022, 58(11): 1519-1526.
[6] 范国华, 缪克松, 李丹阳, 夏夷平, 吴昊. 从局域应力/应变视角理解异构金属材料的强韧化行为[J]. 金属学报, 2022, 58(11): 1427-1440.
[7] 陈瑞润, 陈德志, 王琪, 王墅, 周哲丞, 丁宏升, 傅恒志. Nb-Si基超高温合金及其定向凝固工艺的研究进展[J]. 金属学报, 2021, 57(9): 1141-1154.
[8] 周红伟, 白凤梅, 杨磊, 陈艳, 方俊飞, 张立强, 衣海龙, 何宜柱. 1100 MPa级高强钢的低周疲劳行为[J]. 金属学报, 2020, 56(7): 937-948.
[9] 杨杰, 王雷. 核电站DMWJ中材料拘束的影响与优化[J]. 金属学报, 2020, 56(6): 840-848.
[10] 于家英, 王华, 郑伟森, 何燕霖, 吴玉瑞, 李麟. 热浸镀锌高强汽车板界面组织对其拉伸断裂行为的影响[J]. 金属学报, 2020, 56(6): 863-873.
[11] 易红亮,常智渊,才贺龙,杜鹏举,杨达朋. 热冲压成形钢的强度与塑性及断裂应变[J]. 金属学报, 2020, 56(4): 429-443.
[12] 朱健, 张志豪, 谢建新. 基于原位TEM拉伸的稀土H13钢塑性形变行为和断裂机制[J]. 金属学报, 2020, 56(12): 1592-1604.
[13] 刘杨,王磊,宋秀,梁涛沙. DD407/IN718高温合金异质焊接接头的组织及高温变形行为[J]. 金属学报, 2019, 55(9): 1221-1230.
[14] 周丽,张鹏飞,王全兆,肖伯律,马宗义,于涛. B4C/6061Al复合材料热压缩断裂行为的多尺度研究[J]. 金属学报, 2019, 55(7): 911-918.
[15] 李一哲, 龚宝明, 刘秀国, 王东坡, 邓彩艳. 面外拘束效应对单边缺口拉伸试样断裂韧性的影响[J]. 金属学报, 2018, 54(12): 1785-1791.