摇摆晶体法研究六角密堆单晶体中的位错结构(英文) |
Y.Hao;F.Mucklich;G.Petzow |
Max-Planck-InstitutfurMetallforschung;InstitutfurWerkstoffwissenschaft;Pulverme-tallurgischesLaboratiorium;Heisenbergstr;5;70569Stuttgart;Germany;InstitutefurWerkstoffwissenschafternUniversitatdesSaarlandes;66041Saarbrucken;Max-Planck-InstitutfurMetallfor |
|
INVESTIGATION OF THE DISLOCATION STRUCTURE IN HCP SINGLE CRYSTALS BY MEANS OF THE ROCKING CRYSTAL METHOD |
Y.Hao and G.Petzow (Max-Planck-Institut fur Metallforschung; Institut fur Werkstoffwissenschaft; Pulverme-tallurgisches Laboratiorium; Heisenbergstr. 5; 70569 Stuttgart; Germany)F.Mucklich (Institute fur Werkstoffwissenschaftern Universitat des Saarlandes; 66041 Saarbrucken) |
引用本文:
Y.Hao;F.Mucklich;G.Petzow. 摇摆晶体法研究六角密堆单晶体中的位错结构(英文)[J]. 金属学报, 1997, 33(2): 198-206.
,
,
.
INVESTIGATION OF THE DISLOCATION STRUCTURE IN HCP SINGLE CRYSTALS BY MEANS OF THE ROCKING CRYSTAL METHOD[J]. Acta Metall Sin, 1997, 33(2): 198-206.
1 M.Wilkens, Phys.Status.Solidi.(a) 2 (1970) 359. 2 M.V.Laue, Xray Interkrence (Akademische Verlagsgesellschaft, Leipzig, 1941 ). 3 P.Klimanek, in Annual Reporl 1986 on Nuclear Physics and Applications. ZfK-Publ. 621, ZfKRossendorf 1987. 4 M.A.Krivoglaz and K.P.Ryaboshshapka, Fiz. Met. Metalloved 15 (1963) 18. 5 M.A.Krivoglaz, K.P.Ryaboshshapka and R.I.Barabash, Fis. Met. Metalloved 30 (1970) 1134. 6 O.N.Grigoryev, K.P.Ryaboshapka and N.A.Stel'mashenko, Fiz. Met. Metalloved 67 (1989) 311. 7 R.I.Barabash, M.A.Krivoglaz and K.P.Ryaboshshapka, Fic. Met. Metalloved. 41 (1976) 33. 8 Aldinger and G.Petzow, Beryllium Sci. Technol. 7 (1979) 107. 9 Y.Hao, Dissertation (Max-Planck-Institut, Stuttgart, 1996). 10 C.Brocker et al., Nucl. Instrum. Methodf Phys. Res. A290 (1990) 303. 11 F.Milcklich, Y.Hao and G.Petzow, Proc. Euromat '95, Assoz. Ital. di Metallurgia, Milano, 4 (1995) 305. 12 F.Mhcklich, H.Oettel and G.Petzow, Z.Metallk. 84 (1993) 419. 13 F.Mhcklich and G.Petzow, Development of Beryllium Single Crystal Material .hr Monochromator Applications, in: Mineral Processing and Extractive Metallurgy Review, Beryllium -Issue, Gordon andBreach, New York, (1993) 193. 14 C.May, P.Klimanek and A.Magerl, Nucl. Instrum. Method. Phys. Res. A357 (1995) 511. 15 A.K.Freund, Nucl. Instrum. Method. 7 (1974) 541. 16 A.K.Freund, NucI. Instrum. Method. Phys. Res. A238 (1985) 570.3 |
|