纳米晶体材料的研究现状
卢柯;周飞
中国科学院金属研究所快速凝固非平衡合金国家重点实验室;沈阳;110015;中国科学院金属研究所快速凝固非平衡合金国家重点实验室;沈阳;110015
RECENT RESEARCH PROGRESS ON NANOCRYSTALLINE MATERIALS
LU Ke; ZHOU Fei (State Key Laboratory for RSA; Institute of Metal Research;Chinese Academy of Sciences; Shenyang 110015)
引用本文:

卢柯;周飞. 纳米晶体材料的研究现状[J]. 金属学报, 1997, 33(1): 99-106.
, . RECENT RESEARCH PROGRESS ON NANOCRYSTALLINE MATERIALS[J]. Acta Metall Sin, 1997, 33(1): 99-106.

全文: PDF(868 KB)  
摘要: 本文综述国内外在纳米晶体材料研究领域的最新研究进展,包括纳水晶体材料的制备、微观结构特证、热稳定性、结构性能关系及纳米品体材料的应用
关键词 : 纳米晶体材料,  制备,  微观结构,  性能    
Abstract:Polycrystalline materials with grains sizes in the nanometer region (typically less than 100 nm), termed nanocrystalline materials, have been intensively investigated in the past several years. Much improvement has been made in the field of both fundamental understanding and practical applications of this type of materials. This article reviews the present state of the art in this field. The current status of research and development on the synthesis,microstructure, structural instability, and properties of nanocrystalline materials will be summarized. Further consideations of the development and applications of this new class of materials will also be presented.
Key words: nanocrystalline materials    synthesis    microstructure    properties
收稿日期: 1997-01-18     
基金资助:国家自然科学基金;;中国科学院”百人计划”资助
1Gleiter H Prog Mater Sci,1989; 33: 223
2Suryanarayana C Inter Mater Rev,1995;40: 41
3 Lu K Mater Sci Eng Roports,1996;16;161
4Koch C C. Nanostr Marer,1993;2:109
5Erb U, El-Sherik A M,Palumbo G,AustK T. Nanostr Mater,1993; 2: 383
6 Oehring M,Appel F,Pfullmann Th Bormann R.Appl Phys Lett,1995;66:941
7 He L,Ma E J M ater Res, 1996;11:72
8 He L,Ma E.Nanostr Mater,1996;7 347
9Zhou F, Sheng H W,Lu K to be published
10 Rittner M N,Sanders P G,Weertman J R.Nanostr Mater,1997 to be published
11 Erb U.Nanostr Mater 1995 6: 533
12 Inoue A Zhang T,Nishiyama N,Ohba K,Masumoto T.Mater Sci Eng,1994;A179/A180:210
13 Kawamura Y,Kato H,Inoue A.Appl Phys Lett,1995;67:2008
14 Thomas G J,Siegel R W,Eastman J A Scr Metall Mater,1990;24:201
15 Ganapathi S K,Rigney D AScr Metall Mater,1990;24:1675
16 Li D X Ping D H,Ye H Q,Qin X Y,Wu X J.Mater Letters,1993;18:29
17 Wang J,Wolf D,Phillpot S R Phil Mng A,1996;73:517
18 Keblinsxi P Phillpot S R,Wolf D Nanostr,1997;to be published
19 Lu K,Luck R,Predel B Scr Metall Mater,1993;28:1387
20 Lu K,et al.to be published
21 Terwillinger C D,Chiang Y M MRS Symp Proc,1993;289:15
22 Birringer R,Krill C E,Klingel M Phil Mag Letters,1995;72:71
23 Zhang H Y,Hu Z Q,Lu K J Phys:Condens Matter,1995; 7: 5327
24 Zhao Y H,Lu K to be published
25 Zhang K,Alexandrov I V, Valiev R Z, Lu K J Appl Phys 1996;in print
26 Gunther B,Kumpmann A Kunze H D.Scr Metall Mater,1992;27 83
27 Lu K Nanostr Mater,1993; 2A: 643
28 Lu K,Dong Z F,Lang D Luck R Acta Mater, 1997 to be published
29 Sun N X Lu K Phys Rev B 1996;in print
30 Erb U.(Private Communication)
31 Shen T D,Koch C C,Tsui T Y,Pharr G M J Mater Res,1995;10:2892
32 Lu K,Sui M L Acta Metall Mater,1995;43:3325
33 Siegel R W,Fougere G E Nanostr Mater,1995; 6 205
34卢柯,刘学东,胡壮麒。材料研究学报,1994 8: 385
35 Zhang H Y,Hu Z Q,Lu K.J App Phys,1995;772811,J Mater Res,1997;in print
36 Yan D S, Shi J L,Qin H B,Zheng Y S Gao L.Nanostr Mater,1997;to be published
37 Cheung C, Wood D Erb U In:sufyanarayana C, singh J,Froes F H eds, Processing and Properties of Nanocrystalline Materials,The Minerals,Metals & Materials Society,1996
[1] 张雷雷, 陈晶阳, 汤鑫, 肖程波, 张明军, 杨卿. K439B铸造高温合金800℃长期时效组织与性能演变[J]. 金属学报, 2023, 59(9): 1253-1264.
[2] 张健, 王莉, 谢光, 王栋, 申健, 卢玉章, 黄亚奇, 李亚微. 镍基单晶高温合金的研发进展[J]. 金属学报, 2023, 59(9): 1109-1124.
[3] 宫声凯, 刘原, 耿粒伦, 茹毅, 赵文月, 裴延玲, 李树索. 涂层/高温合金界面行为及调控研究进展[J]. 金属学报, 2023, 59(9): 1097-1108.
[4] 王磊, 刘梦雅, 刘杨, 宋秀, 孟凡强. 镍基高温合金表面冲击强化机制及应用研究进展[J]. 金属学报, 2023, 59(9): 1173-1189.
[5] 郑亮, 张强, 李周, 张国庆. 增/降氧过程对高温合金粉末表面特性和合金性能的影响:粉末存储到脱气处理[J]. 金属学报, 2023, 59(9): 1265-1278.
[6] 陈礼清, 李兴, 赵阳, 王帅, 冯阳. 结构功能一体化高锰减振钢研究发展概况[J]. 金属学报, 2023, 59(8): 1015-1026.
[7] 刘伟, 陈婉琦, 马梦晗, 李恺伦. 聚变堆用W在等离子体作用下的辐照损伤行为研究进展[J]. 金属学报, 2023, 59(8): 986-1000.
[8] 丁桦, 张宇, 蔡明晖, 唐正友. 奥氏体基Fe-Mn-Al-C轻质钢的研究进展[J]. 金属学报, 2023, 59(8): 1027-1041.
[9] 李景仁, 谢东升, 张栋栋, 谢红波, 潘虎成, 任玉平, 秦高梧. 新型低合金化高强Mg-0.2Ce-0.2Ca合金挤压过程中的组织演变机理[J]. 金属学报, 2023, 59(8): 1087-1096.
[10] 袁江淮, 王振玉, 马冠水, 周广学, 程晓英, 汪爱英. Cr2AlC涂层相结构演变对力学性能的影响[J]. 金属学报, 2023, 59(7): 961-968.
[11] 司永礼, 薛金涛, 王幸福, 梁驹华, 史子木, 韩福生. Cr添加对孪生诱发塑性钢腐蚀行为的影响[J]. 金属学报, 2023, 59(7): 905-914.
[12] 吴东江, 刘德华, 张子傲, 张逸伦, 牛方勇, 马广义. 电弧增材制造2024铝合金的微观组织与力学性能[J]. 金属学报, 2023, 59(6): 767-776.
[13] 刘俊鹏, 陈浩, 张弛, 杨志刚, 张勇, 戴兰宏. 高熵合金的低温塑性变形机制及强韧化研究进展[J]. 金属学报, 2023, 59(6): 727-743.
[14] 张德印, 郝旭, 贾宝瑞, 吴昊阳, 秦明礼, 曲选辉. Y2O3 含量对燃烧合成Fe-Y2O3 纳米复合粉末性能的影响[J]. 金属学报, 2023, 59(6): 757-766.
[15] 郭福, 杜逸晖, 籍晓亮, 王乙舒. 微电子互连用锡基合金及复合钎料热-机械可靠性研究进展[J]. 金属学报, 2023, 59(6): 744-756.