| 铸锭凝固行为的数值模拟 |
| 陈卫德;郑贤淑;金俊泽 |
| 大连理工大学 |
|
| NUMERIC AL SIMULATION OF SOLIDIFYING BEHAVIOUR OF CAST INGOT |
| CHEN Weide;ZHENG Xianshu;JIN Junze (Dalian University of Technology;Dalian 116023)(Foundry Research Centre;Dalian University of Technologr;Dalian 116023)(Manuscript received 1995-07-29;in revised form 1995-11-02) |
引用本文:
陈卫德;郑贤淑;金俊泽. 铸锭凝固行为的数值模拟[J]. 金属学报, 1996, 32(10): 1023-1026.
,
,
.
NUMERIC AL SIMULATION OF SOLIDIFYING BEHAVIOUR OF CAST INGOT[J]. Acta Metall Sin, 1996, 32(10): 1023-1026.
| 1BennonWD,IncroperaFP.IntJHeatMassTransf,1987;30:21612BennonWD,incroperaFP.IntJHeatMassTransf,1987;30:21713BennonWD,IncroperaFP.MetallTrans,1987;18B:6114PrescottPJ,IncroperaFP.MetallTrans,1991;22B:5295陈卫德.大连理工大学博士学位论文,1994 |
|