| Ni对C-B_4C-SiC复合材料显微结构与性能的影响 |
| 黄启忠;杨巧勤;杜海清;黄伯云;吕海波 |
| 中南工业大学;湖南大学 |
|
| EFFECT OF Ni ON MICROSTRUCTURE AND PROPERTIES OF C-B_4C-SiC COMPOSITE |
| HUANG Qizhong; YANG Qiaoqin; DU Haiqing; HUANG Boyun';LU Haibo(Institute of Powder Metallurgy Research; Central South University of Technology; Changsha 410083)(Hunan University; Changsha 410082)(Manuscript received 1994-11-04) |
引用本文:
黄启忠;杨巧勤;杜海清;黄伯云;吕海波. Ni对C-B_4C-SiC复合材料显微结构与性能的影响[J]. 金属学报, 1995, 31(19): 337-340.
,
,
,
,
.
EFFECT OF Ni ON MICROSTRUCTURE AND PROPERTIES OF C-B_4C-SiC COMPOSITE[J]. Acta Metall Sin, 1995, 31(19): 337-340.
| 1李杰.碳素,1993;64(4):122MichioInagaki.Carbon,1991;29(3):2873小川一太郎,山本孝义,获尾刚,吉田久良,小林和夫.业协会志,1986;94(4):4094黄启忠,肖汉宁,石强,陈永南,杜海清.陶瓷研究,1994;9(1):205黄启忠,石强,肖汉宁,周新国,杜海清.中国陶瓷,1994;6(2):1 |
|