| 定向凝固Ni_3Al-Mo基合金高温氧化研究 |
| 叶长江;李铁藩;沈嘉年;毛晓禹 |
| 中国科学院金属腐蚀与防护研究所腐蚀科学开放实验室 |
|
| HIGH TEMPERATURE OXIDATION BEHAVIOR OF DS Ni_3Al-Mo BASE ALLOY |
| YE Changjiang;LI Tiefan;SHEN.Jianian;MAO Xiaoyu;(Corrosion Science Lab.;Institute of Corrosion and Protection of Metals; Chinese Academy of Sciences;Shenyang 110015)(Manuscript received 23 August; 1993;in revised form 26 October;1993) |
引用本文:
叶长江;李铁藩;沈嘉年;毛晓禹. 定向凝固Ni_3Al-Mo基合金高温氧化研究[J]. 金属学报, 1994, 30(1): 44-48.
,
,
,
.
HIGH TEMPERATURE OXIDATION BEHAVIOR OF DS Ni_3Al-Mo BASE ALLOY[J]. Acta Metall Sin, 1994, 30(1): 44-48.
| 1韩雅芳,李孙华.金属间化合物,北京:机械工业出版社,1992:702TanignchiS,ShibataT,TsuruokaH,OxidMet,1986;26:13孙超,郭建亭,李辉,管恒荣.中国腐蚀与防护学报,1990;10:1714KubaschewskiO,HopkinsBE,OxidationofMetalsandAlloys,London,1962:2455KuenzlyJD,DouglassDL,OxldMet,1974;8:1396BrennerSS,J.ElectrochemSoc,1955;102:77T著,马志春译,耐热扩散涂层,北京:国防工业出版社,1988:2638SimnadM,SplinersA,JMetals,1955;7:10119TedmonCS,JElectrochemSoc.1966;113:766 |
|