| 晶体取向对铝单晶在循环形变过程中的应力响应、摩擦应力和反馈应力的影响 |
| 夏月波;张天宜;邓钧 |
| 中国科学院金属研究所;副研究员;沈阳(110015);中国科学院金属研究所材料疲劳与断裂国家重点实验室;沈阳工业大学 |
|
| EFFECT OF ORIENTATION ON STRESS RESPONSE, FRICTION STRESS AND BACK STRESS DURING CYCLIC DEFORMATION IN AI SINGLE CRYSTALS. |
| XIA Yuebo; ZHANG Tianyi (State Key Laboratory for Fracture and Failure of Materials; Institute of Metal Research; Academia Sinica; Shenyang) DENG Jun (Shenyang Polytechnical University) |
引用本文:
夏月波;张天宜;邓钧. 晶体取向对铝单晶在循环形变过程中的应力响应、摩擦应力和反馈应力的影响[J]. 金属学报, 1992, 28(8): 42-48.
,
,
.
EFFECT OF ORIENTATION ON STRESS RESPONSE, FRICTION STRESS AND BACK STRESS DURING CYCLIC DEFORMATION IN AI SINGLE CRYSTALS.[J]. Acta Metall Sin, 1992, 28(8): 42-48.
1 Laird C, Charsley P, Mughrabi H. Mater Sci Eng, 1986; 81: 433 2 Mughrabi H. Mater Sci Eng, 1978; 33: 207 3 Cheng A S, Laird C. Mater Sci Eng, 1981; 51: 111 4 Abel A, Wilkelm M, Gerold V. Mater Sci Eng, 1979; 37: 187 5 Vorren O, Ryum N. Acta Metall, 1988; 36: 1443 6 Chicois J, Fougeres R, Guichon G, Hamel A, Vincent A. Acta Metall, 1986; 34: 2157 7 陈贤芬,林栋梁.金属学报,1984;20:A169 8 Vorren O, Ryum N. Acta Metall, 1987; 35:855 9 Xia Y B, Wang Z G, Wang R H. Phys Status Solidi, 1990; a120: 125 10 Winter A T. Philos Mag, 1974; 30:719 11 Finney J M, Laird C. Philos Mag, 1978; 33:207 12 Kuhlmann-Wilsdorf D, Laird C. Mater Sci Eng, 1979; 37: 111 13 Jin N Y. Acta Metall, 1989; 37: 2055 14 Yamamoto A, Imura T. In: Ashby M F, Bullough R, Hartley C S, Hirth J P eds., Dislocation Modelling of Physical Systems, Proc Int Conf, Gainesville, Florida, June 22-27, 1980, Oxford: Pergamon, 1981w |
|