| 渗碳钢在裂纹萌生前的疲劳行为 |
| 陈铁群;I.VERPOEST;A.DERUYTTERE |
| 武汉工学院;比利时Katholieke大学;比利时Katholieke大学 |
|
| FATIGUE BEHAVIOR OF CARBURIZED STEEL BEFORE CRACK INITIATION |
| CHEN Tjequn Wuhan Institute of Technolgy; VERPOEST I; DERUYTTERE A Department of Metallurgy; Katholieke Universiteit; Leuven; Belgium |
引用本文:
陈铁群;I.VERPOEST;A.DERUYTTERE. 渗碳钢在裂纹萌生前的疲劳行为[J]. 金属学报, 1991, 27(4): 64-66.
,
,
.
FATIGUE BEHAVIOR OF CARBURIZED STEEL BEFORE CRACK INITIATION[J]. Acta Metall Sin, 1991, 27(4): 64-66.
1 Chen T. Fatigue Crack Propagation in Carburized Steel, Ph D Thesis, K. U., Leuven, Belgium, 1988 2 Polak J, Klesnil M, Lukas P. Mater Sci Eng, 1977; 28: 109--117 3 Feltner C E, Laird C. Acta Metall, 1967; 15: 1621--1632 4 Lukas P. Symp on Fatigue CsVTS, Praha, 1961: 100 5 McGrath J T, Bratina W J, Philos Mag, 1965; 12: 1293--1305 6 Feltner C E. Philes Mag, 1965; 12: 1229--1248# |
|