| Ni_3Al-Mo高温复合材料的拉伸特性 |
| 王成国;菊池潮美 |
| 山东工业大学;讲师;日本京都大学 |
|
| TENSILE BEHAVIOUR OF HIGHTEMPERATURE Ni_3 Al-Mo COMPOSITE |
| WANG Chengguo Shandong Polytechnic University; Jinan; KIKUCHI Shiomi Kyoto University; Japan |
引用本文:
王成国;菊池潮美. Ni_3Al-Mo高温复合材料的拉伸特性[J]. 金属学报, 1991, 27(2): 135-139.
,
.
TENSILE BEHAVIOUR OF HIGHTEMPERATURE Ni_3 Al-Mo COMPOSITE[J]. Acta Metall Sin, 1991, 27(2): 135-139.
1 王成国,菊池潮美,兴津贵隆,小岩昌宏.材料,1990;39(7) :878 2 Tartaglia J M, Stoloff N S. Metall Trans, 1981; 12A: 1119 3 Funk W, Blank E. Metall Trans, 1988; 19A: 987 4 Sprenger H, Richter H, Nickl J J. J Mater Sci. 1976; 11: 2075 5 Nemoto M, Honda T, Nakagawa Y G, Saiga Y, Suto H. Trans Jpn Inst Met, 1980; 21: 495 6 三岛良积,岩田修一.新材料开发材料设计学.东京:社,1985:21 7 山口正治,马越佑吉.金属间化合物.东京:日刊工业新闻社,1986:29 8 Thornton P H, Davies R G, Johnston T L. Metall Trans, 1970; 1: 207 |
|