| 金属-氧化物扩散障的理论计算 |
| 孙碧武;管恒荣;孙晓峰;李铁藩 |
| 中国科学院金属研究所;博士研究生;中国科学院金属研究所;中国科学院金属研究所;中国科学院金属腐蚀与防护研究所 |
|
| A MODEL OF METAL-OXIDE DIFFUSION BARRIER |
| SUN Biwu;GUAN Hengrong;SUN Xiaofeng Institute of Metal Research; Academia Sinica; Shenyang; LI Tiefan Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang |
引用本文:
孙碧武;管恒荣;孙晓峰;李铁藩. 金属-氧化物扩散障的理论计算[J]. 金属学报, 1991, 27(2): 108-113.
,
,
,
.
A MODEL OF METAL-OXIDE DIFFUSION BARRIER[J]. Acta Metall Sin, 1991, 27(2): 108-113.
1 孙碧武,管恒荣,孙晓峰,李铁藩.金属学报,1990;26:B 401 2 Luthre K L. J Vac Sci Technol, 1985; A3: 2574--2577 3 Lesage B, Huntz A M. Scr Metall, 1980; 14: 1143--1146 4 Szekely J, Evans J W, Sohn H Y. Gas-Solid Reaction, New York: Academic, 1976: 27 5 Sun Biwu, Guan Hengrong, Sun Xiaofeng, Li Tiefan. International Symposium on High Temperature Corrosion and Protection. June 26--30, 1990, Shenyang, China, 1990: 6 Oezisik M N,俞昌铭主译.热传导.北京:高等教育出版社,1983:350--353 7 Green A, Swindells N. Mater Sci Technol, 1985; 1: 101--103 8 汪复兴.金属物理.北京:机械工业出版社,1981:165--167 9 Guan Hengrong, Sun Biwu.Sun Xiaofeng,Li Tiefan. International Symposium on High Temperature Corrosion and Protection, June 26--30, 1990. Shenyang, Chins, 1990: |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|