| Fe(Ⅲ)-H_2SO_4-Na_2SO_4水溶液体系的离子平衡 |
| 伍志春;于淑秋 |
| 中国科学院化工冶金研究所;助理研究员北京100080;中国科学院化工冶金研究所 |
|
| IONIC EQUILIBRIA IN Fe(Ⅲ)-H_2SO_4-Na_2SO_4 AQUEOUS SOLUTION SYSTEM |
| WU Zhichun;YU Shuqiu Institute of Chemical Metallurgy; Academia Sinica; Beijing |
引用本文:
伍志春;于淑秋. Fe(Ⅲ)-H_2SO_4-Na_2SO_4水溶液体系的离子平衡[J]. 金属学报, 1991, 27(1): 83-88.
,
.
IONIC EQUILIBRIA IN Fe(Ⅲ)-H_2SO_4-Na_2SO_4 AQUEOUS SOLUTION SYSTEM[J]. Acta Metall Sin, 1991, 27(1): 83-88.
1 Dousma J. Den Ottelander D. De Bruyn P L. J Inorg Nucl Chem, 1979; 41: 1565 2 Lee C K, Tavlarides L L. Polyhedron, 1985; 4: 47 3 伍志春,于淑秋,陈家镛.金属学报,1990;26(3) :B 4 陈家镛,于淑秋,伍志春.湿法冶金中铁的分离及其利用,(第2章),北京:冶金工业出版社(待出版) 5 Hasinoff B B. Can J Chem 1976; 54: 1820 6 Jost A. Ber Bunsenges Phys Chem. 1976; 80: 316 7 Funahashi S, et al. Inorg Chem, 1983; 22: 2070 8 Swaddle T W, Merbach A E. Inorg Chem, 1981; 20: 4212S |
|