| Fe表面多种离子注入层的研究 |
| 王佩璇;孙晓冬;张建伟;张国光;卢浩林;杨启法;徐虬 |
| 北京科技大学;北京科技大学;北京科技大学;北京科技大学材料物理系;北京100083;原子能研究院;原子能研究院;原子能研究院 |
|
| MICROSTRUCTURE OF CARBURIZED LAYERS ON IRON SURFACE IMPLANTED WITH Ni~+, Mo~+ AND B~+ OR THEIR COMBINATIONS |
| WANG Peixuan;SUN Xiaodong;ZHANG Jianwei;ZHANG Guoguang University of Science and Technology Beijing; LU Haolin. YANG Qifa;XU Qiu Institute of Atomic Energy; Beijing |
引用本文:
王佩璇;孙晓冬;张建伟;张国光;卢浩林;杨启法;徐虬. Fe表面多种离子注入层的研究[J]. 金属学报, 1991, 27(1): 130-136.
,
,
,
,
,
,
.
MICROSTRUCTURE OF CARBURIZED LAYERS ON IRON SURFACE IMPLANTED WITH Ni~+, Mo~+ AND B~+ OR THEIR COMBINATIONS[J]. Acta Metall Sin, 1991, 27(1): 130-136.
1 Lu Haolin, Shu Huiqin, Mei Chen et al. Vacuum, 1989; 39: 187 2 Knapp J A. Follstaedt D M, Doyle B L. Nucl Instrum Methods Phys Res. 1985; B7/8: 38 3 Singer I L. Vacuum, 1984; 34: 853 4 Rauschenbach B. Nucl Instrum Methods phys Res, 1986; B15: 756 5 Hohmuth K, Rauschenbach B, Kolitsch A et al. Nucl Instrum Methods, 1983; 209/210: 249 6 Linker G. Mater Sci Eng, 1985; 69: 105 7 Follstaedt D M. Nucl Instrum Methods Phys Res, 1985; B7/8: 11 8 Vardiman R G. Bolster R N, Singer I L. In: Picraux S T, Choyke W J eds. Metastable Materials Formation by Ion Implantation, Proceedings of the Materials Research Society Annual Meeting, 16--18 November, 1981, Boston, Massachusetts, USA, New York: North Holland, 1982: 269M |
|
Viewed |
|
|
|