晶粒大小对双相不锈钢的强度和氢致开裂的影响 |
何建宏;唐祥云;陈南平 |
讲师;武汉(430074);华中理工大学机械二系金属材料教研室;清华大学;清华大学 |
|
INFLUENCE OF GRAIN SIZE ON STRENGTH AND HYDROGEN INDUCED CRACKING OF DUPLEX STAINLESS STEELS |
HE Jianhong;TANG Xiangyun;CHEN Nanping Huazhong University of Science and Technology; Wuhan Tsinghua University; Beijing Department of Materials Science and Engineering; Huazhong University of Science and Technology; Wuhan 430074 |
引用本文:
何建宏;唐祥云;陈南平. 晶粒大小对双相不锈钢的强度和氢致开裂的影响[J]. 金属学报, 1990, 26(4): 27-31.
,
,
.
INFLUENCE OF GRAIN SIZE ON STRENGTH AND HYDROGEN INDUCED CRACKING OF DUPLEX STAINLESS STEELS[J]. Acta Metall Sin, 1990, 26(4): 27-31.
1 横川清志,福山诚司,工藤清勝.日本金属学会志,1984;48:901--910 2 何建宏,唐祥云,陈南平.金属学报,1989;25:A37--41 3 何建宏,唐祥云,陈南平.机械工程材料,1988;12(5) :8--10 4 福山诚司,横川清志,工藤清勝,大谷南海男.日本金属学会志,1982;46:1193--1199, |
|