| 双相不锈钢中裂纹尖端塑性变形行为的透射电镜原位观察 |
| 姚可夫;唐迺泳;陈南平 |
| 清华大学;清华大学;清华大学 |
|
| IN SITU OBSERVATION OF CRACK TIP DEFORMATION IN A DUPLEX STAINLESS STEEL |
| YAO Kefu;TANG Naiyong;CHEN Nanping Tsinghua University |
引用本文:
姚可夫;唐迺泳;陈南平. 双相不锈钢中裂纹尖端塑性变形行为的透射电镜原位观察[J]. 金属学报, 1989, 25(3): 57-62.
,
,
.
IN SITU OBSERVATION OF CRACK TIP DEFORMATION IN A DUPLEX STAINLESS STEEL[J]. Acta Metall Sin, 1989, 25(3): 57-62.
1 Rice J R, Rosengren G F. J Mech Phys Solids, 1968; 16: 1 2 Hutchinson J W. J Mech Phys Solids, 1968; 16: 13 3 Gardner R N, Wilsdoif H G F. Metall Trans, 1980; 11A: 653 4 Ohr S M. Mater Sci Eng, 1985; 72: 1 5 张以增,戴蜀娟,邹鸿承,苗丕峰,理化检验(物理分册),1985;22(5) :19 6 姚可夫,唐迺泳,陈南平.第五届全国断裂力学会议文集,桂林,1988:156 |
|