| 裂纹在珠光体钢中的近门槛区扩展 |
| 邓蓉英;周爱华;蒋怀庆;李春秀;张立卿;孙宇田 |
| 中国科学院力学研究所;中国科学院力学研究所;中国科学院力学研究所;中国科学院力学研究所;中国科学院力学研究所;中国科学院力学研究所 |
|
| FATIGUE CRACK PROPAGATION NEAR THRESHOLD IN PEARLITIC STEEL |
| DENG Rongying;ZHOU Aihua;JIANG Huaiqing;LI Chunxiu;ZHANG Liqing;SUN Yutian Institute of Mechanics; Academia Sinica; Beijing |
引用本文:
邓蓉英;周爱华;蒋怀庆;李春秀;张立卿;孙宇田. 裂纹在珠光体钢中的近门槛区扩展[J]. 金属学报, 1989, 25(3): 63-69.
,
,
,
,
,
.
FATIGUE CRACK PROPAGATION NEAR THRESHOLD IN PEARLITIC STEEL[J]. Acta Metall Sin, 1989, 25(3): 63-69.
1 Miller L E, Smith G C. J Iron Steel Inst, 1970; 228: 998 2 Rosenfield A R, Hahn G T, Embury J D. Metall Trans, 1972; 3: 2797 3 Porter D A, Easterling K E, Smith G D W. Acta Metall, 1978; 26: 1405 4 Vosikovsky O. Eng Fract Mech, 1979; 11: 595 5 邓蓉英,马远福,机械强度,1982;1:22 6 邓蓉英,李禾,于桂清.金属学报,1984;20:A76 7 Elber W. ASTM STP 486, 1971: 230] |
|