| Nd_2(Fe_(1-x)M_x)_(14)B(M=C,Si)合金的磁性 |
| 邢峰;江潮;何文望 |
| 讲师;北京大学物理系;北京大学物理系;北京大学物理系 |
|
| MAGNETIC PROPERTIES OF Nd_2(Fe_(1-x)M_x)_(14)B(M=C, Si) ALLOYS |
| XING Feng;JIANG Chao;HO Wenwang Department of Physics; Peking University |
引用本文:
邢峰;江潮;何文望. Nd_2(Fe_(1-x)M_x)_(14)B(M=C,Si)合金的磁性[J]. 金属学报, 1988, 24(5): 420-424.
,
,
.
MAGNETIC PROPERTIES OF Nd_2(Fe_(1-x)M_x)_(14)B(M=C, Si) ALLOYS[J]. Acta Metall Sin, 1988, 24(5): 420-424.
1 Herbst J F, Croat J J, Yelon W B. J Appl Phys, 1985; 57: 4086 2 Matsuura Y. Hirosawa S, Yamamo to H, Fujimura S, Sagawa M. Appl Phys Lett, 1985; 46: 308 3 Yang Y C (杨应昌), Ho W W (何文望), Chen H Y (陈海英), Wang J (王进), Lan J (兰健). J Appl Phys, 1985; 57: 4118 4 Abache C, Oesterreicher H. J Appl Phys, 1986; 57: 1114 5 Liuingston J D. Proc 8th Int Wokshop on Rare-Earth Magnets and their Applioations 1985: 423 6 杨应昌,何文望,陈海英,邢峰,兰健,中国稀土学报,1985;3(2) :34 7 Sucksmith W, Thompson J E. Proc Roy Soc London, Ser. A, 1954; 225: 362 8 Koon N C, Das B N, Rubinstein M, Tyson J. J Appl Phys, 1985; 57: 4091 9 Givord D, Li H S, Perrier de la Bathie R. Solid State Commun, 1984; 51: 857 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|