| 评价溶质元素细化晶粒能力的参数 |
| 韩青有;胡汉起 |
| 北京钢铁学院铸造教研室;北京钢铁学院 |
|
| A PARAMETER FOR EVALUATING ABILITY OF GRAIN REFINEMENT OF SOLUTE ELEMENTS |
| HAN Qingyou;HU Hanqi Beijing University of Iron and Steel Technology |
引用本文:
韩青有;胡汉起. 评价溶质元素细化晶粒能力的参数[J]. 金属学报, 1988, 24(5): 392-396.
,
.
A PARAMETER FOR EVALUATING ABILITY OF GRAIN REFINEMENT OF SOLUTE ELEMENTS[J]. Acta Metall Sin, 1988, 24(5): 392-396.
1 胡汉起.金属凝固,冶金工业出版社,1985:89 2 Winegard W C, Chalmers B. Trans Am Soc Met, 1954; 46: 1214 3 Genolers R. J Inst Met, 1926; 35: 259 4 Papapetron A Z. Krist, 1935; A92: 89 5 大野笃美,唐彦斌,张正德译.金属凝固学,机械工业出版社,1983:88 6 韩青有,胡汉起.北京钢铁学院学报,1985;(1) :1 7 张兴中.溶质分配系数的研究,北京钢铁学院硕士研究生论文,1985 8 Smithells C J. Metals Reference Book, 5th ed., London: Butterworths, 1976 9 Rinaldi M D, Sharp R M, Flemings M C. Metall Trans. 1972; 3: 3133 10 胡汉起,钟雪友,力航.金属学报,1984;20:A247 11 胡汉起,钟雪友,韩青有,金属学报,1987;23:A176{ |
|