| Fe-Cr-P非晶合金镀层腐蚀特性的研究 |
| 陈晓怡;郭大侠;罗泾源 |
| 北京钢铁学院;北京钢铁学院;北京钢铁学院物化教研室;副教授 |
|
| CORROSION BEHAVIOR OF AMORPHOUS Fe-Cr-P ALLOY PLATING FOILS |
| CHEN Xiaoyi;GUO Daxia Beijing University of Iron and steel TechnologyLUO Jingyuan Associate Professor;Depertment of Physicat Chemistry;Beijing University of Iron and Steel Technology |
引用本文:
陈晓怡;郭大侠;罗泾源. Fe-Cr-P非晶合金镀层腐蚀特性的研究[J]. 金属学报, 1988, 24(2): 204-206.
,
,
.
CORROSION BEHAVIOR OF AMORPHOUS Fe-Cr-P ALLOY PLATING FOILS[J]. Acta Metall Sin, 1988, 24(2): 204-206.
1 Hashimoto K. Asami K, Naka M, Masumoto T. Corros Sci, 1979; 19: 857--867 2 奈贺正明,桥本功二,增本健.日本金属学会志,1974;38:835--841 3 Naka M, Hashimoto K, Masumoto T. Corrosion, 1976; 32: 146--152 4 Masumoto T, Hashimoto K, Ann Rev Mater Sci, 1978; (8) : 215--233 5 陈晓怡,罗泾源.北京钢铁学院学报,1988;10(1) |
|